UBE UPIMOL® SA101 Heat-Resistant Polyimide Shape

Category Polymer , Thermoset , Polyimide, TS
Manufacturer UBE
Trade Name UPIMOL®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF UBE UPIMOL® SA101 Heat-Resistant Polyimide Shape.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: UPIMOL® SA101 is an excellent heat-resistant polyimide shape, based on Biphenyl tetracarboxilic dianhydride(BPDA) originally developed by UBE. UPIMOL® SA101 has improved high durability for oxygen plasma, vacuum degassing properties, low water absorption and good processability. Heat distortion temperature is 470°C.Applications: Semiconductor production equipment partsVacuum equipment partsPrecisely processed partsHeat and chemical resistant gaskets and sealing materialsFeatures: Super high heat resistance (Heat distortion temperature: 470°C)Excellent plasma resistanceLow out gasGood processabilityVery low impuritiesLow water absorptionInformation provided by UBE.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
23°C; ASTM D792
Water Absorption 0.030 %
0.030 %
23°C for 24 hr; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 115
115
ASTM D785
Tensile Strength, Ultimate 110 MPa
16000 psi
ASTM D638
47.0 MPa

@Temperature 260 °C
6820 psi

@Temperature 500 °F
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
3.0 %

@Temperature 260 °C
3.0 %

@Temperature 500 °F
ASTM D638
Flexural Strength 135 MPa
19600 psi
ASTM D790
51.0 MPa

@Temperature 260 °C
7400 psi

@Temperature 500 °F
ASTM D790
Flexural Modulus 7.50 GPa
1090 ksi
ASTM D790
3.60 GPa

@Temperature 260 °C
522 ksi

@Temperature 500 °F
ASTM D790
Izod Impact, Notched 0.200 J/cm

@Temperature 23.0 °C
0.375 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Limiting Pressure Velocity 3.53 MPa-m/sec
101000 psi-ft/min
0.1 m/sec; S45C
Taber Abrasion, mg/1000 Cycles 20
20
ASTM D1044
Thermal Properties Metric English Comments
CTE, linear 35.0 µm/m-°C

@Temperature 25.0 - 450 °C
19.4 µin/in-°F

@Temperature 77.0 - 842 °F
ASTM E233
Thermal Conductivity 0.407 W/m-K
2.82 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 470 °C
878 °F
Heat Distortion Temp, Load Unknown; ASTM D648
Decomposition Temperature 623 °C
1150 °F
10% Weight Loss Temp
Electrical Properties Metric English Comments
Volume Resistivity 1.90e+16 ohm-cm
1.90e+16 ohm-cm
ASTM D257
Surface Resistance 8.50e+16 ohm
8.50e+16 ohm
ASTM D257
Dielectric Constant 3.7
3.7
ASTM D150
Dielectric Strength 22.7 kV/mm
577 kV/in
Breakdown Voltage; ASTM D149
Dissipation Factor 0.0013
0.0013
ASTM D150
Arc Resistance 135 sec
135 sec
23°C; ASTM D495
Descriptive Properties Value Comments
Durability for O2 Plasma 6.6 micro gr/cm<sup>2</sup>hr
Etching Rate Test at 145-150°C
Vacuum Degassing 5.5 x 10<sup>-4</sup> Torr x l/sec x cm<sup>2</sup>
TDS Analysis at 200°C
7.6 x 10<sup>-4</sup> Torr x l/sec x cm<sup>2</sup>
TDS Analysis at 300°C