| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced, Flame Retardant |
| Manufacturer | Unitika |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Unitika BV2120 PA66, Flame Retardant, Conditioned.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.33 g/cc | 0.0480 lb/in³ | ISO 1183 |
| Moisture Absorption at Equilibrium | 1.5 % | 1.5 % | 50% RH; ISO 62 |
| Linear Mold Shrinkage, Flow | 0.015 cm/cm @Thickness 3.20 mm |
0.015 in/in @Thickness 0.126 in |
|
| Linear Mold Shrinkage, Transverse | 0.017 cm/cm @Thickness 3.20 mm |
0.017 in/in @Thickness 0.126 in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 96 | 96 | ISO 2039 |
| Tensile Strength at Break | 50.0 MPa | 7250 psi | ISO 527-1/-2 |
| Elongation at Break | 4.8 % | 4.8 % | ISO 527-1/-2 |
| Tensile Modulus | 1.60 GPa | 232 ksi | ISO 527-1/-2 |
| Flexural Strength | 66.0 MPa | 9570 psi | ISO 178 |
| Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
| Charpy Impact Unnotched | 5.60 J/cm² | 26.6 ft-lb/in² | ISO 179-1 |
| Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179-1 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-2 |
| Flammability, UL94 | V-0 @Thickness 0.750 mm |
V-0 @Thickness 0.0295 in |