Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Unitika E-RUNG60 Ultra high-rigidity PA6, Dry

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Unitika
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unitika E-RUNG60 Ultra high-rigidity PA6, Dry.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ultra high-rigidityInformation provided by Unitika Ltd.
Physical Properties Metric English Comments
Density 1.73 g/cc
0.0625 lb/in³
ASTM D792
Moisture Absorption at Equilibrium 0.70 %
0.70 %
50% RH
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 248 MPa
36000 psi
ASTM D638
Elongation at Break 4.1 %
4.1 %
ASTM D638
Flexural Strength 358 MPa
51900 psi
ASTM D790
Flexural Modulus 18.1 GPa
2630 ksi
ASTM D790
Izod Impact, Notched 1.49 J/cm
2.79 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 222 °C
432 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 249 °C
480 °F
ASTM D648