Wieland 1101 Wilaform Gold

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy
Manufacturer Wieland
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland 1101 Wilaform Gold.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Hard yellow gold alloy with good extensibility. Universally applicable in decoration manufacturing.Applications: casting, chainsDental
Physical Properties Metric English Comments
Density 10.9 g/cc
0.394 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 110
110
HV5; glowed
Tensile Strength, Ultimate 420 MPa
60900 psi
Elongation at Break 35 %
35 %
Thermal Properties Metric English Comments
Melting Point 820 - 880 °C
1510 - 1620 °F
Solidus 820 °C
1510 °F
Liquidus 880 °C
1620 °F
Component Elements Properties Metric English Comments
Copper, Cu 40.76 %
40.76 %
Gold, Au 37.5 %
37.5 %
Silver, Ag 8.5 %
8.5 %
Zinc, Zn 13.24 %
13.24 %
Processing Properties Metric English Comments
Processing Temperature 600.0 °C
1112 °F
Cuvette Temp
Casting Temperature 980 - 1080 °C
1800 - 1980 °F
Descriptive Properties Value Comments
Color yellow