| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Fiber Filled, Flame Retardant |
| Manufacturer | Zhejiang Juner New Materials Co. |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Zhejiang Juner PA-A1 Flame-Retardant & Glass Reinforced, Non-Halogen PA66.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.32 g/cc | 0.0477 lb/in³ | GB/1033 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 60.0 MPa | 8700 psi | GB/1040 |
| Flexural Strength | 100 MPa | 14500 psi | GB/9341 |
| Charpy Impact Unnotched | 2.00 J/cm² | 9.52 ft-lb/in² | IS0179-1:2000 |
| Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | IS0179-1:2000 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 140 °C | 284 °F | GB1634 |
| Flammability, UL94 | V-2 | V-2 | GB/T2408 |
| Flammability Test | 12 | 12 | Glow-Wire Test (sec); GB/5169.11 |
| 13 | 13 | Flame Remainder (%); GB/9345 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 500 V | 500 V | GB/4207 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 255 - 285 °C | 491 - 545 °F | |
| Mold Temperature | 80.0 - 120 °C | 176 - 248 °F | |
| Drying Temperature | 110 °C @Time 7200 sec |
230 °F @Time 2.00 hour |
Vacuum Pressure, -0.08 MPa |
| 120 °C @Time 18000 sec |
248 °F @Time 5.00 hour |
Chute Hot-Wind | |
| 120 °C @Time 21600 sec |
248 °F @Time 6.00 hour |
Horizontal Oven | |
| Injection Pressure | 65.0 - 120 MPa | 9430 - 17400 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Speed of Shoot, % | 45-95 |