Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® LC-0522-A LDPE Extrusion Resin Excellent sealability, High drawdown, High adhesion, Good barrier, High stiffness, Good abrasion resistanceApplications: Milk cartons, Paperboard containers, Liquid packaging, Woven fabrics, Lumber .. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® LF-Y320-D Fractional Melt LDPE Film Resin Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D1505 |
SABIC HP0722N Low Density Polyethylene for Blown Film Product Description: HP0722N is a Low Density Polyethylene grade suitable for producing medium duty films and contains no slip or antiblock additives. It yields good toughness and optical properti.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Chevron Phillips 2118 Liner Grade Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: High Impact Strength, Good Heat Seal Characteristics, Good Processability, Low GelsApplications:Trash bags and other linersProcessing Conditions: Extruder 6.3.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 0.5 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-421 LDPE Power Cable Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable polyethylene homopolymer designed as an electrical grade base resin.Applications: A base resin for fully formulated crosslinkable me.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | Exxon Method |
ExxonMobil Exceed™ 377D60 LDPE/Hexene Tough Premium Film Resin, 3 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 377D60 resin exhibit excellent impact strength and b.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ISO 1183 |
Borealis Bormed™ LE6601-PH LDPE for Pharmaceutical Blow Molding Bormed LE6601-PH is a LD-polyethylene produced in a high-pressure process intended for blow molding of soft and flexible packages for pharmaceutical products.Bormed LE6601-PH can be used in "blow-fi.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D1505 |
UBE F022 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D1505 |
UBE F222NH Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D1505 |
UBE F522N Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ISO 1183 |
Borealis FG5223 Linear Low Density Polyethylene FG5223 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant and anti-block additives. This grade is developed for production of lamination film. FG5223 has good heat.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | base resin; ISO 1183/ISO 1872-2 |
Borealis LE4201R Polyethylene Insulation Compound, Crosslinkable LE4201R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications LE4201R is intended for insulation of XLPE power cables with rated voltages up.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | base resin; ISO 1183/ISO 1872-2 |
Borealis Supercure™ LE8201R Polyethylene Insulation Compound, Crosslinkable Supercure™ LE8201R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Supercure™ LE8201R is recommended for use with Supercure™ LE8280 as shielding.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ExxonMobil Method |
ExxonMobil LD 637.LI Molding, Extrusion and Compounding Resin Product Description: LD 637.LI is a high melt index LDPE homopolymer intended for injection molding or compounding applications requiring high flow. It is ideal for tamper-evident, tear-to-open clos.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin (European Grade) Product Description: LD 165 series are LDPE grades, offering high strength combined with medium optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoTherm.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | |
Dow DOWLEX™ 2070D Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2070D Polyethylene resin is a fully formulated linear low density polyethylene resin offering high strength and low gel properties for blown film food packaging applications. DOWLEX 2070D r.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | |
Dow LDPE 501I Low Density Polyethylene, Clear Film Grade DOW LDPE 501I, a barefoot resin used for bakery film and other packaging applications that require optical clarity. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food con.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | |
Dow LDPE 530A Low Density Polyethylene, Blown Film Grade DOW LDPE 530A resin, is a general purpose barefoot blown film extrusion resin with excellent drawdown and processability for packaging applications. This material complies with U.S.FDA regulation 21.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | |
Dow LDPE 640I Low Density Polyethylene, Liner Film Grade DOW LDPE 640I resin is a barefoot general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. This material complies with U.S.FDA regulation 21 CFR .. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | |
Dow LDPE 752A Low Density Polyethylene, Film Grade DOW LDPE 752A resin is a drawdown film resin for thin gauge applications such as garment films. It contains high levels of both slip and antiblock additives. This material complies with U.S.FDA regu.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM-D792 |
Braskem F2022/0 LDPE Cast Film Extrusion Polyethylene LDPE F2022/0 has excellent sealing characteristics and optical properties with well balanced mechanical properties. Its applications include: general purpose which require no additives; shrink film.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Braskem PB681/59 LDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Lamination film; general purpose. Information provided by Braskem |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM-D792 |
Braskem TX7012 LDPE Blown Film Extrusion Polyethylene TX7012 is a low-density polyethylene (LDPE) with medium molecular weight and good processability in traditional extruders with good mechanical properties and productivity, ensuring uniform thickness.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D-1505 |
Bapolene® 213B Polyethylene, Extrusion Grade Bapolene 213B is a low density polyethylene for molding, extrusion and foaming applications. It contains slip and complies with US FDA regulation 21 CFR 177.1520 (Olefin polymers), paragraph (c)2.1.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D-1505 |
Bapolene® 270F Low Density Polyethylene Film Extrusion Resin Bapolene® 270F is an LDPE for blown film requiring superior clarity. It contains 1600 ppm antiblock and 725 ppm slip additives. This product meets the Food and Drug Administration requirements of .. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | |
BASF Ethyl Acrylate Formula: C5H8O2CAS: 140-88-5Description: Acrylic acid ester suitable for the production of polymers and as a feedstock for syntheses.Applications: Ethyl acrylate forms homopolymers and copolymers. .. |
|||
Density | 0.922 - 0.925 g/cc | 0.0333 - 0.0334 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | base resin; ISO 1183/ISO 1872-2 |
Borealis Supercure™ LS4201S Polyethylene Insulation Compound, Crosslinkable Supercure™ LS4201S is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: Supercure™ LS4201S is intended for insulation of XLPE High Volta.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Huntsman PE8010 Specialty Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent draw down and machinability.Applications: Film extrusion: gel free film applications.FDA Notes: Conforms to FDA regulation 21 CFR 1.. |