Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.89 g/cc | 0.285 lb/in³ | |
Latrobe LSSâ„¢ H14 Tool Steel (ASTM H14) TLS H14 tool steel is a 5%-chromium hot work steel to which tungsten has been added for improved high-temperature properties and heat resistance. It is a deep-hardening, airhardening
steel that exh.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | |
Latrobe TNWâ„¢ ASTM M10 High Speed Steel TNW is an M10 type high speed steel with a composition that combines the high toughness of a high-molybdenum steel and the excellent wear resistance provided by the 2%
vanadium content. TNW is popul.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | |
Schmolz + Bickenbach UGIMA 303 UX® Stainless Steel Bar Description: 303 UGIMA UX® is an improved machining grade produced only by Ugitech, providing the ultimate level of machinability available in an austenitic stainless steel. 303 UGIMA UX® feat.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | |
Schmolz + Bickenbach UGIMA® 303 HD Stainless Steel Bar Description: 303 UGIMA HD™ is a low sulfur version of Ugitech’s improved machining 303 grade. It is designed to provide better metallurgical performance with respect to weldability, corros.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | |
Schmolz + Bickenbach UGIMA® 303 Stainless Steel Bar Description: 303 UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 303, except with respect to machinability. 303 UGIMA® repre.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 301 Austenitic Stainless Steel, 1/2 Hardened Type 301 is a chromium-nickel stainless steel that provides high strength and good ductility with chromium and nickel contents lowered to increase the work hardening range. This permits higher tens.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 301 Austenitic Stainless Steel, 1/4 Hardened Type 301 is a chromium-nickel stainless steel that provides high strength and good ductility with chromium and nickel contents lowered to increase the work hardening range. This permits higher tens.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 301 Austenitic Stainless Steel, Annealed Type 301 is a chromium-nickel stainless steel that provides high strength and good ductility with chromium and nickel contents lowered to increase the work hardening range. This permits higher tens.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 301 Austenitic Stainless Steel, Full Hardened Type 301 is a chromium-nickel stainless steel that provides high strength and good ductility with chromium and nickel contents lowered to increase the work hardening range. This permits higher tens.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 302 Austenitic Stainless Steel, 1/2 Hardened Types 302 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 302 Austenitic Stainless Steel, 1/4 Hardened Types 302 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 302 Austenitic Stainless Steel, 1/8 Hardened Types 302 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 302 Austenitic Stainless Steel, 3/4 Hardened Types 302 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 304 Austenitic Stainless Steel, 1/2 Hardened Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 304L Austenitic Stainless Steel, Annealed Type 304L is a very common variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled. Lower carbon 304L minimizes chromium ca.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 304L Austenitic Stainless Steel, Full Hardened Type 304L is a very common variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled. Lower carbon 304L minimizes chromium ca.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 304 Austenitic Stainless Steel, 1/4 Hardened Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 304 Austenitic Stainless Steel, 1/8 Hardened Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 304 Austenitic Stainless Steel, 3/4 Hardened Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 304 Austenitic Stainless Steel, Annealed Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 304L Austenitic Stainless Steel, 1/4 Hardened Type 304L is a very common variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled. Lower carbon 304L minimizes chromium ca.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | As Annealed |
Eagle Brass 304L Austenitic Stainless Steel, 1/8 Hardened Type 304L is a very common variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled. Lower carbon 304L minimizes chromium ca.. |
|||
Density | 7.89 g/cc @Temperature 399 °C |
0.285 lb/in³ @Temperature 750 °F |
soft annealed |
Bohler-Uddeholm UDDEHOLM VANADIS 30 AISI M2 + Co SUPERCLEAN 3 Powder Metallurgical Cold Work Tool Steel Uddeholm Vanadis 30 is a Co high alloyed powder metallurgy high speed steel corresponding to AISI M3:2 + Co. The high compressive strength, 67 HRC, and good abrasive wear resistance makes Uddeholm V.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | |
Carlson Nitronic® 50® Austenitic Stainless Steel General DescriptionNitronic 50 is a nitrogen-strengthened austenitic stainless steel that possesses corrosion resistance superior to 316, 316L, 317 and 317L plus approximately twice the yield streng.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | soft annealed condition |
Assab Steels ASP 60 Cold Work Steel ASP 60 is a W-Mo-V-Co alloyed PM high speed steel characterized by:Highest wear resistanceMaximum compressive strengthGood through hardening propertiesGood toughnessGood dimensional stability on hea.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | |
Carpenter AerMet® 100 Aged at 875°F An alloy providing high hardness and strength combined with exceptional ductility and toughness. This alloy should be considered for aircraft and aerospace structural components requiring high stren.. |
|||
Density | 7.89 g/cc @Temperature 400 °C |
0.285 lb/in³ @Temperature 752 °F |
soft annealed condition |
Assab Steels ASP 30 Cold Work Steel ASP 30 is a W-Mo-v-Co alloyed PM high speed steel characterized by:High wear resistanceHigh compressive strength at high hardnessGood through hardening propertiesGood toughnessGood dimensional stabi.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | |
Schmolz + Bickenbach Holder Block Plastic Mold Steel Description: Holder Block is a modified AISI-4130 material with higher chromium and molybdenum content specifically designed holder steel for molds and dies and The material is forged on a 5000 ton.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | |
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar Description: 304/304L UGIMA® is the next generation of improved high machinability grades from Ugitech. The UGIMA® grades have redefined high machinability stainless steels, showing improvements o.. |
|||
Density | 7.89 g/cc | 0.285 lb/in³ | |
Latrobe LSS™ S1 Shock-Resisting Tool Steel (ASTM S1) TLS S1 Shock-Resisting tool steel is a medium-carbon steel which combines moderate hardness with good impact toughness. It is a deep-hardening, oil-hardening steel designed for shock and impact load.. |