Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.09 - 1.46 g/cc | 0.0394 - 0.0527 lb/in³ | Average value: 1.23 g/cc Grade Count:23 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Density | 1.05 - 1.46 g/cc | 0.0379 - 0.0527 lb/in³ | Average value: 1.34 g/cc Grade Count:126 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Density | 0.980 - 1.46 g/cc | 0.0354 - 0.0527 lb/in³ | Average value: 1.05 g/cc Grade Count:296 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Density | 1.03 - 1.46 g/cc | 0.0372 - 0.0527 lb/in³ | Average value: 1.11 g/cc Grade Count:301 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Density | 1.42 - 1.46 g/cc | 0.0513 - 0.0527 lb/in³ | ISO R 1184 |
Fainplast Compounds RI 52 Rigid PVC, Injection Molding Fittings for building trade |
|||
Density | 1.39 - 1.46 g/cc | 0.0502 - 0.0527 lb/in³ | 254 Hardener |
Lord Adhesives Versilok® 262 / 254 Acrylic Adhesive LORD Versilok® 262/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alumi.. |
|||
Density | 1.39 - 1.46 g/cc | 0.0502 - 0.0527 lb/in³ | 254 Hardener |
Lord Adhesives Versilok® 262B / 254 Acrylic Adhesive LORD Versilok® 262B/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alum.. |
|||
Density | 1.39 - 1.46 g/cc | 0.0502 - 0.0527 lb/in³ | 254 Hardener |
Lord Adhesives Versilok® 265 / 254 Acrylic Adhesive LORD Versilok® 265/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alumi.. |
|||
Density | 1.42 - 1.46 g/cc | 0.0513 - 0.0527 lb/in³ | ISO R 1184 |
Fainplast Compounds RKS 321 Rigid PVC, Antishock Extrusion Lead Free Outdoor antishock profiles |
|||
Density | 1.42 - 1.46 g/cc | 0.0513 - 0.0527 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 80/1 Flexible PVC, Sheathing Sheath coaxial TV Cable |
|||
Density | 1.42 - 1.46 g/cc | 0.0513 - 0.0527 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 86 Flexible PVC, Sheathing General purposes |
|||
Density | 1.42 - 1.46 g/cc | 0.0513 - 0.0527 lb/in³ | ISO R 1183 |
Fainplast Compounds FR 90 Flexible PVC, Insulation General purposes |
|||
Density | 1.42 - 1.46 g/cc | 0.0513 - 0.0527 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 72 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | 1.42 - 1.46 g/cc | 0.0513 - 0.0527 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 90/R Flexible PVC, Flame Retardant Sheathing Hydrocarbon resistant |
|||
Density | 1.42 - 1.46 g/cc | 0.0513 - 0.0527 lb/in³ | ISO R 1184 |
Fainplast Compounds GK 0185/R Flexible PVC, Flame Retardant Sheathing Lead Free Oil and hydrocarbon resistant sheath (90°C) |
|||
Density | 1.42 - 1.46 g/cc | 0.0513 - 0.0527 lb/in³ | ISO R 1183 |
Fainplast Compounds GK 86/R Flexible PVC, Flame Retardant Sheathing Lead Free Hydrocarbon resistant |
|||
Density | 1.42 - 1.46 g/cc | 0.0513 - 0.0527 lb/in³ | ISO R 1184 |
Fainplast Compounds GS 78 Flexible PVC, Electrical Plugs Plugs |
|||
Density | 1.42 - 1.46 g/cc | 0.0513 - 0.0527 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 78 Flexible PVC, Injection Molding for Technical Items Plugs |
|||
Density | 1.42 - 1.46 g/cc | 0.0513 - 0.0527 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 76/7 Flexible PVC, Sheathing Medium flexibility |
|||
Density | 1.42 - 1.46 g/cc | 0.0513 - 0.0527 lb/in³ | ISO R 1185 |
Fainplast Compounds GK 0474 Flexible PVC, Flame Retardant Sheathing Lead Free General purposes |
|||
Density | 1.42 - 1.46 g/cc | 0.0513 - 0.0527 lb/in³ | ISO R 1184 |
Fainplast Compounds HG 80/2 Flexible PVC, Sheathing for High Temperatures Operating temperature 90°C |
|||
Density | 1.42 - 1.46 g/cc | 0.0513 - 0.0527 lb/in³ | ISO R 1183 |
Fainplast Compounds HL 92/1 Flexible PVC, Insulation for High Temperatures Operating temperature 105°C, flame retardant, oil resisting |
|||
Density | 1.42 - 1.46 g/cc | 0.0513 - 0.0527 lb/in³ | ISO R 1184 |
Fainplast Compounds KL 92/3 Flexible PVC, Insulation for High Temperatures Lead Free Operatine temperature 105°C |
|||
Density | 1.40 - 1.46 g/cc | 0.0506 - 0.0527 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATS 1613-R Phenolic Molding Nylon and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackMedium flow Applications:Railwa.. |
|||
Density | 1.38 - 1.46 g/cc | 0.0499 - 0.0527 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATS 766 Phenolic Molding Chopped cotton fabric Filler, Compression Molded Characteristics:High impact strengthGlossy surfaceLow shrinkageGood sliding propertiesColor-BrownMedium flowApplications:Cog wheelsCastor wheelsBush bearingsPulleysWelding rod handlesTextile bobbins.. |
|||
Density | 1.22 - 1.46 g/cc | 0.0441 - 0.0527 lb/in³ | Average value: 1.36 g/cc Grade Count:8 |
Overview of materials for Nylon 66/6, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Density | 1.27 - 1.46 g/cc | 0.0459 - 0.0527 lb/in³ | Average value: 1.32 g/cc Grade Count:15 |
Overview of materials for Nylon 66, 40% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in.. |
|||
Density | 0.886 - 1.46 g/cc | 0.0320 - 0.0527 lb/in³ | Average value: 0.906 g/cc Grade Count:153 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |
|||
Density | 0.970 - 1.46 g/cc | 0.0350 - 0.0527 lb/in³ | Average value: 1.06 g/cc Grade Count:237 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |
|||
Density | 1.32 - 1.46 g/cc | 0.0477 - 0.0527 lb/in³ | Average value: 1.38 g/cc Grade Count:7 |
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Aramid Fiber Filled". Each property range of values reported is minimu.. |