Physical Properties Metric English Comments
Density 0.938 - 1.01 g/cc
0.0339 - 0.0365 lb/in³
Average value: 0.954 g/cc Grade Count:266
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum..
Density 0.990 - 1.01 g/cc

@Temperature 20.0 °C
0.0358 - 0.0365 lb/in³

@Temperature 68.0 °F
Silikony Polskie Polsil E5S Silicone Emulsion
POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. ..
Density 0.990 - 1.01 g/cc

@Temperature 20.0 °C
0.0358 - 0.0365 lb/in³

@Temperature 68.0 °F
Silikony Polskie Polsil E1 Silicone Emulsion
POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. ..
Density 0.990 - 1.01 g/cc

@Temperature 20.0 °C
0.0358 - 0.0365 lb/in³

@Temperature 68.0 °F
Silikony Polskie Polsil E2 Silicone Emulsion
POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. ..
Density 0.990 - 1.01 g/cc

@Temperature 20.0 °C
0.0358 - 0.0365 lb/in³

@Temperature 68.0 °F
Silikony Polskie Polsil E3 Silicone Emulsion
POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. ..
Density 0.990 - 1.01 g/cc

@Temperature 20.0 °C
0.0358 - 0.0365 lb/in³

@Temperature 68.0 °F
Silikony Polskie Polsil E5 Silicone Emulsion
POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. ..
Density 0.950 - 1.01 g/cc
0.0343 - 0.0365 lb/in³
Average value: 0.967 g/cc Grade Count:14
Overview of materials for Polypropylene with 10% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are ..