Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.938 - 1.01 g/cc | 0.0339 - 0.0365 lb/in³ | Average value: 0.954 g/cc Grade Count:266 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |
|||
Density | 0.959 - 1.01 g/cc | 0.0346 - 0.0364 lb/in³ | |
Lord Adhesives 551 Very Low Viscosity, Adhesive Thinner, Medium Cure Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Density | 0.990 - 1.01 g/cc @Temperature 20.0 °C |
0.0358 - 0.0365 lb/in³ @Temperature 68.0 °F |
|
Silikony Polskie Polsil E5S Silicone Emulsion POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. .. |
|||
Density | 0.990 - 1.01 g/cc @Temperature 20.0 °C |
0.0358 - 0.0365 lb/in³ @Temperature 68.0 °F |
|
Silikony Polskie Polsil E1 Silicone Emulsion POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. .. |
|||
Density | 0.990 - 1.01 g/cc @Temperature 20.0 °C |
0.0358 - 0.0365 lb/in³ @Temperature 68.0 °F |
|
Silikony Polskie Polsil E2 Silicone Emulsion POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. .. |
|||
Density | 0.990 - 1.01 g/cc @Temperature 20.0 °C |
0.0358 - 0.0365 lb/in³ @Temperature 68.0 °F |
|
Silikony Polskie Polsil E3 Silicone Emulsion POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. .. |
|||
Density | 0.990 - 1.01 g/cc @Temperature 20.0 °C |
0.0358 - 0.0365 lb/in³ @Temperature 68.0 °F |
|
Silikony Polskie Polsil E5 Silicone Emulsion POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. .. |
|||
Density | 0.950 - 1.01 g/cc | 0.0343 - 0.0365 lb/in³ | Average value: 0.967 g/cc Grade Count:14 |
Overview of materials for Polypropylene with 10% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are .. |