Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Trelleborg Emerson & Cuming Eccobond® 64C Two-Component Nickel Filled Electrically Conductive Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive , Epoxy, Electrically Conductive
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Eccobond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Eccobond® 64C Two-Component Nickel Filled Electrically Conductive Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming 64C Eccobond® Two-Component Nickel Filled Electrically Conductive Epoxy AdhesiveTwo component, nickel filled, electrically conductive epoxy adhesive. Room temperature cure. Good balance of low cost and high conductivity. Recommended for use where exposure to salt water causes silver based systems to corrode. Cure Type: Room Temperature Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 3.20 g/cc
0.116 lb/in³
Mechanical Properties Metric English Comments
Adhesive Bond Strength 5.52 MPa
800 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.020 ohm-cm
0.020 ohm-cm
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 100 °C
0.500 hour

@Temperature 212 °F
60.0 min

@Temperature 65.0 °C
1.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Dark Grey
Viscosity Thixotropic (Mixed, 25°C)
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved