Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.10 g/cc | 0.293 lb/in³ | |
Kennametal Stellite Nucalloy® 453 High-Silicon Nickel-Base Hardfacing Alloy Applications include chemical control valves, nuclear globe valves, nuclear gate valves, nuclear sliding parts, and pressure bars for plywood cutters.Nucalloy® alloys are unique, patented, high-s.. |
|||
Density | 8.10 g/cc | 0.293 lb/in³ | |
Kennametal Stellite Nucalloy® 488 High-Silicon Nickel-Base Hardfacing Alloy Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinations of hardness and toughness, similar to the cobalt base alloys . B.. |
|||
Density | 8.10 g/cc | 0.293 lb/in³ | |
Kennametal Stellite Nucalloy® 488V High-Silicon Nickel-Base Hardfacing Alloy Applications include diesel engine valves, and injection mold screws.Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinati.. |
|||
Density | 8.12 g/cc | 0.293 lb/in³ | |
Indium Corp. Indalloy 281-338 Bismuth-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.10 g/cc | 0.293 lb/in³ | |
LATI Latimass 82-03 D080 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
Special Metals INCONEL® Alloy 601 A nickel-chromium alloy with an addition of aluminum for outstanding resistance to oxidation and other forms of high-temperature corrosion. It also has high mechanical properties at elevated temper.. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
Special Metals NILO® Alloy 36 Low-Expansion Alloy Inflection point 220°C. A nickel-iron low-expansion alloy containing 36% nickel. It maintains nearly constant dimensions over the range of normal atmospheric temperatures, and has a low coeffic.. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy Inflection point 370°C. A nickel-iron controlled-expansion alloy containing 42% nickel. It has a low and nominally constant coefficient of thermal expansion from room temperature to about 570Â.. |
|||
Density | 8.10 g/cc | 0.293 lb/in³ | |
Wall Colmonoy COLMONOY® 6 Nickel-Base Hard-Surfacing Alloy With Chromium Boride Description: The original, nickel-base hard-surfacing alloy, containing diamond-like chromium borides (and carbides). Extremely resistant to wear, especially under corrosive conditions. Low coeffi.. |
|||
Density | 8.10 g/cc | 0.293 lb/in³ | |
Goodfellow Evanohm® Precision Resistance Nickel Alloy Electrical resistance alloy with a very low temperature coefficient of resistivityInformation provided by Goodfellow. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
Crucible Steel CPM® REX® M35HCHS High Speed Steel, AISI M35 CPM REX M35HCHS is a 5% cobalt modification of M2 high speed steel used almost exclusively for hobs and other gear cutting tools where higher red hardness is required. Made by the Crucible Particle .. |
|||
Density | 8.10 g/cc | 0.293 lb/in³ | |
Bohler-Uddeholm BÖHLER S390 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
Density | 8.10 g/cc | 0.293 lb/in³ | |
Bales Mold Service Nibore® Electroless Nickel - Boron Nitride Mold Coating Nibore® is an electroless nickel phosphorus coating that incorporates boron nitride particles in a co-deposited nickel matrix. This unique process is formulated to produce a uniformly dispersed bor.. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
California Fine Wire Stablohm 800 Nickel, Chromium, Aluminum, and Copper Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.11 g/cc | 0.293 lb/in³ | |
Carlson C 601 Nickel-Chromium-Iron Alloy General DescriptionCarlson Alloy C 6021 is a nickel-chromium alloy, developed specifically for high –temperature service. This alloy exhibits outstanding resistance to both cyclic and static oxida.. |
|||
Density | 8.10 g/cc | 0.293 lb/in³ | |
Bohler-Uddeholm BÖHLER S500(m42) High Speed Steel Description: Cobalt Molybdenum high speed steel processing high hardness, excellent cutting properties, high red hardness and good toughness. BOHLER S500 is also available in the special grade ISORA.. |
|||
Density | 8.12 g/cc | 0.293 lb/in³ | |
AIM 40Bi/60Sn Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Density | 8.10 g/cc | 0.293 lb/in³ | |
AIM 54Sn/26Pb/20In Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Density | 8.12 g/cc | 0.293 lb/in³ | |
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.15 mm Strip Heat Treated 843°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
Density | 8.12 g/cc | 0.293 lb/in³ | |
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.35 mm Strip Heat Treated 760°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
Density | 8.12 g/cc | 0.293 lb/in³ | |
Carpenter Hiperco® Alloy 50 Fe-Co-V Soft Magnetic Alloy, Cold Rolled Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |
|||
Density | 8.10 g/cc | 0.293 lb/in³ | |
Kennametal Stellite Nucalloy® 430 High-Silicon Nickel-Base Hardfacing Alloy Applications include components of chemical processing.Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinations of hardness .. |
|||
Density | 8.12 g/cc | 0.293 lb/in³ | |
Carpenter Hiperco® 50 Fe-Co-V Soft Magnetic Alloy, 0.15 mm Strip Heat Treated 760°C Hiperco® alloy 50 is an iron-cobalt-vanadium soft magnetic alloy which exhibits high magnetic saturation (24 kilogauss), high D.C. maximum permeability, low D.C. coercive force, and low A.C. core l.. |