Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.931 - 0.935 g/cc | 0.0336 - 0.0338 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4133Q (33403) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Tritheva® TN 2020 EVA Copolymer The Tritheva TN 2020 resin is a Ethylene-Vinyl Acetate copolymer (EVA) developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Th.. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 2315 LLDPE Injection Molding Resin
(discontinued **) Features: Low odor, low warpage, fast cycling, high surface gloss, permits light weight lid design, low temperature impact excellent.Data provided by the manufacturer. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ASTM D1505 |
Eastman 5265 LDPE 6.5% EVA Copolymer, Clarity, Ultra-high Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Excellent heat seal characteristics, Good optical properties, Superior impact strength, Low coefficient of friction, Good processability, High Slip, High Ant.. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ASTM D1505 |
Eastman 5267 LDPE 6.5% EVA Copolymer, Clarity, Ultra-high Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Excellent heat seal characteristics, Excellent impact strength, Good optical properties, Good processability, High antiblock, No slipApplications:Laminations.. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ASTM D1505 |
Eastman 5284 LDPE 8% EVA Copolymer, High Clarity, Ultra-High Impact Film Resin
(discontinued **) Resin Type: CopolymerCharacteristics: Excellent Heat Seal Characteristics, Superior Impact Strength, Good Optical Properties, No Slip, High Antiblock, High Coefficient of FrictionApplications:Ice Ba.. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® LD 712.06 Film Resin
(discontinued **) Escorene Ultra LD 712 series is a fraction melt index, 10 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness, particular.. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® NA324009 Low Density Polyethylene (Blow Molding Applications) ApplicationsPETROTHENE NA 324-009 is a low density homopolymer resin intended for blow molding applications. NA 324-009 provides good clarity, toughness and processability. Typical applications in.. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ASTM D1505 |
LyondellBasell Plexar® PX1007 Extrudable Tie-Layer Resin - Anhydride Modified EVA ApplicationsPlexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and .. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ASTM D1505 |
Westlake DA591 9.0% Ethylene Vinyl Acetate Copolymer Westlake DA591 resin is a 9.0% EVA copolymer designed as a tie layer in multi-layered food packaging film. It has excellent clarity, excellent toughness, good resistance to load deformation, and goo.. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | D 1505 |
Westlake EB591 9.0% Ethylene Vinyl Acetate Copolymer Westlake EB591 resin is a 9.0% EVA copolymer designed for ice bags, frozen food bags and other films that require excellent toughness and good heat sealing characteristics. This kosher compliant re.. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ASTM-D1505 |
Westlake Elevate™ EB591 9% EVA Copolymer Westlake EB591 resin is a 9% EVA copolymer designed for films that require excellent toughness and good heat sealing characteristics. This Kosher compliant resin has excellent low temperature brittl.. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ISO 1183 |
Borealis Borstar® FB2310 LLDPE for Film Borstar BF2310 is a high molecular weight low density polyethylene film grade combining good and flexible extrusion behavior, excellent draw down and superior mechanical properties. Film made from .. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ASTM D792 |
DuPont Bynel® 2002 Acid-Modified Ethylene Terpolymer Adhesive Resin Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ FL 00209 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00209 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 270°C (518°F) may cause resin degradation. Machines should always b.. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 157CW Blown Low Density Polyethylene Resin Product Description: LD 157CW offer good mechanical properties as well as excellent opticals.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesAppl.. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 157CW Wire & Cable Low Density Polyethylene Resin Product Description: LD 157CW is a medium density LDPE recommended for the production of Low Voltage power cable insulation, using the on-step silane cross0linking technology. The grade contains a h.. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 380BA Blown Low Density Polyethylene Resin (European Grade) Product Description: LD 380BA offers good toughness and optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: Coextrus.. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ASTM D792 |
Dow AMPLIFY™ EA 101 Ethylene-ethyl Acrylate (EEA) AMPLIFY™ EA 101 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility and imparts low temperature toughness to a wide range of engineering resins. This polymer.. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ASTM D792 |
Dow AMPLIFY™ EA 102 Ethylene-ethyl Acrylate (EEA) AMPLIFY™ EA 102 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility and imparts low temperature toughness to a wide range of engineering resins. This polymer.. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ASTM D792 |
Dow DNDA-1081 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-1081 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ASTM D792 |
Dow DNDA-1149 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-1149 NT 7 is produced using UNIPOL™ PE process technology and is intended for high-speed injection molding applications. Information provided by Dow |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ISO 1183 |
Arkema Group OREVAC® 18350 Grafted Maleic Anhydride Polyethylene OREVAC 18350 is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE and HDPE coating for steel pipeline. It is mainly used in pipe coating to have good adhesion per.. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ISO 1183 |
Arkema Group OREVAC® 18350P Grafted Maleic Anhydride Polyethylene OREVAC 18350P is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE and HDPE coating for steel pipeline. It is mainly used in pipe coating to have good adhesion pe.. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ASTM-D1505 |
Braskem TN2020 EVA General Film Copolymer TN2020 is an Ethylene-Vinyl Acetate (EVA) copolymer developed to mostly meet the needs of the multi-layer packaging segment produced by coextrusion and/or lamination processes. Multilayer structures.. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ASTM-D729 |
Braskem IF33 LLDPE Injection Molding Polyethylene Copolymer IF33 is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high fluidity, good flexibility, .. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ASTM-D792 |
Braskem TS9002 LDPE Blown Film Extrusion Polyethylene TS9022 is a low-density polyethylene (LDPE) developed specially for automatic overwrap packaging. This resin has a combination of high optical properties and excellent stiffness. The incorporated ad.. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | compound; ISO 1183 |
Borealis LE6022 Polyethylene Modified Jacketing Compound LE6022 is a black low density copolymer modified polyethylene compound. It is characterized by excellent crack resistance and mechanical properties and low temperature performance in combination wit.. |
|||
Density | 0.931 g/cc | 0.0336 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 13J7 Octene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity.Applications: Film.Data provided by the manufacturer. |