Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.11 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.03 - 1.11 g/cc
0.0372 - 0.0401 lb/in³
Average value: 1.06 g/cc Grade Count:8
Overview of materials for Nylon 11, Cable Sheathing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o..
Density 1.094 - 1.11 g/cc
0.03952 - 0.0401 lb/in³
B Grade
Kazanorgsintez Diethanolamine, Technical
Production Method: Obtained by ammonia oxyethylation with further rectification. Application: For implementation in the organic synthesis process as a sorbing agent for natural gas treatment; in was..
Density 1.107 - 1.11 g/cc
0.03999 - 0.0401 lb/in³
Fibre Glast 2000 / 2060 System 2000 Epoxy
System 2000 Epoxy Resin is a low viscosity, light amber laminating resin that is designed for fabricating parts and other demanding structural applications. Use this system to maximize the physical ..
Density 1.07 - 1.11 g/cc
0.0387 - 0.0401 lb/in³
RP-0134
Solvay RHODAFAC® AAP Surfactant
Chemical Name: AMYL ACID PHOSPHATE; ORGANIC ACID PHOSPHATE CAS: 71-41-0, 7664-38-2 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: RHODAFAC© AAP imparts excellent..
Density 1.03 - 1.11 g/cc
0.0372 - 0.0401 lb/in³
RP-0549
Solvay RHODATERGE® BCC Surfactant
Description: Rhodaterge® BCC is Surfactant Base for Low Foaming, Highly Alkaline Cleaners (45% solids). Delivers exceptional surface tension reduction in high caustic systems; stable in 50% Sodiu..
Density 0.890 - 1.11 g/cc
0.0322 - 0.0401 lb/in³
Trelleborg Offshore Vikotherm™ 73585 Insulative Elastomer
Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res..
Density 0.978 - 1.11 g/cc
0.0353 - 0.0401 lb/in³
Average value: 1.05 g/cc Grade Count:9
Overview of materials for Silicone Polyurethane, Ether Based
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value..