Polymer Property : Density = 1.34 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.960 - 1.34 g/cc
0.0347 - 0.0484 lb/in³
Average value: 1.07 g/cc Grade Count:42
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a..
Density 1.21 - 1.34 g/cc
0.0437 - 0.0484 lb/in³
Average value: 1.29 g/cc Grade Count:8
Overview of materials for Thermoplastic Polyimide, Unfilled
Density 1.30 - 1.34 g/cc
0.0470 - 0.0484 lb/in³
Fusor 2201
Lord Adhesives Fusor® 2200 / 2201 Urethane Adhesive
Fusor® 2200/2201 is a black equal-mix, twocomponent, paste urethane adhesive system. Fusor 2200/2201 adhesive bonds FRP, SMC, and other plastics with little surface preparation where bond strengt..
Density 1.18 - 1.34 g/cc
0.0426 - 0.0484 lb/in³
Trelleborg Emerson & Cuming Eccobond® 45 Two-Component General Purpose Epoxy Adhesive
Emerson & Cuming 45 Eccobond® Two-Component General Purpose Epoxy AdhesiveFilled, general purpose, room temperature curing, epoxy adhesive and sealant. Flexibility can be adjusted by the amount of ..
Density 1.28 - 1.34 g/cc
0.0462 - 0.0484 lb/in³
Dow BETAMATE™ XW 1185 Epoxy
BETAMATE™ XW 1185 is a one component heat curing Epoxy paste adhesive. The material is readily pumped at ambient temperatures. It shows excellent adhesion to automotive steel and aluminum, is resi..
Density 1.30 - 1.34 g/cc
0.0470 - 0.0484 lb/in³
ISO R 1183
Fainplast Compounds FK 76 Flexible PVC, Insulation Lead Free
General purposes
Density 1.30 - 1.34 g/cc
0.0470 - 0.0484 lb/in³
ISO R 1183
Fainplast Compounds GS 7816 Flexible PVC, Injection Molding for Footwear
Soles for mild climates
Density 1.30 - 1.34 g/cc
0.0470 - 0.0484 lb/in³
ISO R 1183
Fainplast Compounds CL 65 Flexible PVC, Sheathing
General purposes
Density 1.30 - 1.34 g/cc
0.0470 - 0.0484 lb/in³
ISO R 1183
Fainplast Compounds MRK 267 Medical Rigid PVC, Injection Molding
Anti-impact connectors and components
Density 1.30 - 1.34 g/cc
0.0470 - 0.0484 lb/in³
ISO R 1183
Fainplast Compounds PM 5540 Flexible PVC, Extrusion
Gaskets for frames
Density 1.30 - 1.34 g/cc
0.0470 - 0.0484 lb/in³
ISO R 1183
Fainplast Compounds PM 9012 Flexible PVC, Extrusion
Furniture border
Density 1.30 - 1.34 g/cc
0.0470 - 0.0484 lb/in³
ISO R 1184
Fainplast Compounds KL 96/1 Flexible PVC, Insulation for High Temperatures Lead Free
Automotive cables low thickness
Density 1.30 - 1.34 g/cc
0.0470 - 0.0484 lb/in³
ISO R 1183
Fainplast Compounds PM 6045 Flexible PVC, Lead Free
Gaskets for frames
Density 1.30 - 1.34 g/cc
0.0470 - 0.0484 lb/in³
ISO R 1183
Fainplast Compounds FKA 97 Flexible PVC, Flame Retardant Insulation Lead Free
Telephonic insulation
Density 1.30 - 1.34 g/cc
0.0470 - 0.0484 lb/in³
ISO R 1183
Fainplast Compounds PM 8020 Flexible PVC, Lead Free
Covering steel sheaths
Density 1.30 - 1.34 g/cc
0.0470 - 0.0484 lb/in³
ISO R 1183
Fainplast Compounds PM 8030 Flexible PVC, Lead Free
Furniture border