Physical Properties Metric English Comments
Density 1.05 - 1.48 g/cc
0.0379 - 0.0535 lb/in³
Average value: 1.13 g/cc Grade Count:123
Overview of materials for Polypropylene with 30% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are..
Density 1.44 - 1.48 g/cc
0.0520 - 0.0535 lb/in³
ISO R 1184
Fainplast Compounds RH 207/OP Rigid PVC, Antishock Extrusion
Medium antishock satined profiles
Density 1.44 - 1.48 g/cc
0.0520 - 0.0535 lb/in³
ISO R 1184
Fainplast Compounds RH 211/W Rigid PVC, Antishock Extrusion
Various antishock profiles
Density 1.44 - 1.48 g/cc
0.0520 - 0.0535 lb/in³
ISO R 1184
Fainplast Compounds RH 212/W Rigid PVC, Antishock Extrusion
Outdoor antishock profiles
Density 1.44 - 1.48 g/cc
0.0520 - 0.0535 lb/in³
ISO R 1184
Fainplast Compounds RK 912 Rigid PVC, Extrusion Lead Free
Spiral pipes
Density 1.44 - 1.48 g/cc
0.0520 - 0.0535 lb/in³
ISO R 1184
Fainplast Compounds RKS 212/W Rigid PVC, Antishock Extrusion Lead Free
Outdoor antishock profiles
Density 1.44 - 1.48 g/cc
0.0520 - 0.0535 lb/in³
ISO R 1184
Fainplast Compounds RKS 315/W Rigid PVC, Antishock Extrusion Lead Free
Various profiles antishock
Density 1.44 - 1.48 g/cc
0.0520 - 0.0535 lb/in³
ISO R 1184
Fainplast Compounds RKS 320 Rigid PVC, Antishock Extrusion Lead Free
Various profiles, antishock
Density 1.44 - 1.48 g/cc
0.0520 - 0.0535 lb/in³
ISO R 1183
Fainplast Compounds FR 83 Flexible PVC, Insulation
General purposes
Density 1.44 - 1.48 g/cc
0.0520 - 0.0535 lb/in³
ISO R 1184
Fainplast Compounds HG 83 Flexible PVC, Sheathing for High Temperatures
Operating temperature 90°C
Density 1.44 - 1.48 g/cc
0.0520 - 0.0535 lb/in³
ISO R 1184
Fainplast Compounds HGA 84 Flexible PVC, Sheathing for High Temperatures
Operating temperature 90°C
Density 1.44 - 1.48 g/cc
0.0520 - 0.0535 lb/in³
ISO R 1184
Fainplast Compounds HGK 82 Flexible PVC, Sheathing for High Temperatures Lead Free
Operating temperature 90°C
Density 1.44 - 1.48 g/cc
0.0520 - 0.0535 lb/in³
ISO R 1183
Fainplast Compounds CKL 0411/UV Flexible PVC, Sheathing Lead Free
General purposes (anti UV)
Density 1.44 - 1.48 g/cc
0.0520 - 0.0535 lb/in³
ISO R 1183
Fainplast Compounds FR 86/2 Flexible PVC, Insulation
Power cables
Density 1.44 - 1.48 g/cc
0.0520 - 0.0535 lb/in³
ISO R 1183
Fainplast Compounds GS 65/C Flexible PVC, Injection Molding, Lead Free
Mats
Density 1.44 - 1.48 g/cc
0.0520 - 0.0535 lb/in³
ISO 1183
Fainplast Compounds Hax™ HF 224/4 Flame Retardant Polyolefin Cable Compound
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, insulation, high flexibilityInformation provided by Fainplast Compounds
Density 1.44 - 1.48 g/cc
0.0520 - 0.0535 lb/in³
ISO 1183
Fainplast Compounds Hax™ HFX 521 Crosslinkable HFFR Cable Compound
Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Oil resistant sheathingInformation provided by Fainplast C..
Density 1.05 - 1.48 g/cc
0.0379 - 0.0535 lb/in³
Average value: 1.21 g/cc Grade Count:99
Overview of materials for Polyether Ester Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr..
Density 0.895 - 1.48 g/cc
0.0323 - 0.0535 lb/in³
Average value: 0.986 g/cc Grade Count:93
Overview of materials for Ethylene Butyl Acrylate
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp..