Premix Premi-Glas® 1201-10 Polyester SMC  (discontinued **)

Category Polymer , Thermoset , Composite SMC , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Premix Premi-Glas® 1201-10 Polyester SMC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Premi-Glas® 1201-10 is a 10% glass reinforced thermoset Sheet Molding Compound designed for sinks, shower stall bases and wall applications. Key features and benefits are:Supports ANSI 124.2 and CSA B45.5 requirements for flame, smoke and stain resistance. Available in glass contents ranging from 10% - 20%; standard product has 15% reinforcement. High gloss, non-rippling surface appearance on large flat surfaces and deep draw side walls. Excellent as-molded dimensional tolerances. Outstanding moldability and flow in compression process. Standard color is white.Passes ANSI 124.2/ CSA B,45.5 stain resistanceData provided by Premix.
Physical Properties Metric English Comments
Density 1.65 - 1.75 g/cc
0.0596 - 0.0632 lb/in³
ASTM D792
Water Absorption 0.10 - 0.30 %
0.10 - 0.30 %
ASTM D570
Linear Mold Shrinkage 0.00 - 0.0020 cm/cm
0.00 - 0.0020 in/in
Ambient part /mold
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 24.1 - 34.5 MPa
3500 - 5000 psi
ASTM D638
Modulus of Elasticity 7.58 - 8.96 GPa
1100 - 1300 ksi
ASTM D638
Flexural Yield Strength 62.1 - 82.7 MPa
9000 - 12000 psi
ASTM D790
Flexural Modulus 6.89 - 8.96 GPa
1000 - 1300 ksi
ASTM D790
Izod Impact, Notched 2.14 - 3.20 J/cm
4.00 - 6.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.20 - 4.27 J/cm
6.00 - 8.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 204 °C
>= 400 °F
ASTM D648