Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
LNP Lubricomp® PDX-O-90351 Polyphenylene Sulfide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | |
Parker Chomerics CHO-FLEX 601 Conductive Coating CHO-FLEX™ 601 coating is specifically designed for EMI shielding of copper/Kapton flexible circuit laminates and for printing circuits on Kapton film. Upon cure, this coating exhibits excellent adh.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
FKuR Kunststoff Biograde® C 9550 Biodegradable Plastic Compound BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especial.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
Lanxess Pocan® T 7391 000000 PBT + PET, 45% Glass Fiber PBT+PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | |
LATI Larton G/40 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
Lanxess Pocan® BF 8230 000000 PBT, 30% Glass Fiber PBT, 30% glass spheres/glass fibers, injection molding, flame retardant, low tendency to warp, improved surface finish |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP OX90351 PPS LNP LUBRICOMP* OX90351 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PA6/6 GF30 FR BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedAppear.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
Techmer ES HiFill® POM CO 0167 S2 LE Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: Copolymer and Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Verton OX07411 PPS (Asia Pacific) LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON UV00ASU PPA LNP* VERTON* UV00ASU is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: UV Stabilized, Heat Stabilized, Structural. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | Relative Density; ISO 1183 |
Vyncolit X620/1 Novolac Phenolic Glass fiber and graphite filled phenolic molding compound with excellent friction properties.USES: Low friction bearings, video recorder and compact disc parts. Not suitable for applications requir.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183-87 |
Wellman Wellpet® FRGF116-BK1 Polyethylene Terephthalate, 30% Glass Fiber Reinforced, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
Polyram RamSter PE321G6 PET, 30% Glass Fiber, Flame Retardant 30% Glass fiber reinforced, flame retardant V-0 PET for injection molding applications.Information provided by Polyram. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
DSM Arnite® TV4 260 SN PBT-GF30 FR(17) 30% Glass Reinforced, Flame Retardant |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® SK695FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b.. |
|||
Density | 1.67 g/cc @Temperature 23.0 °C |
0.0603 lb/in³ @Temperature 73.4 °F |
DIN 53 479 |
Ensinger TECASINT 1041 Polyimide, 30% MoS2 Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
Eurostar Starpylen HU 70E4 ECR Starpylen HU 70E4 ECR is a Renewable Calcium Carbonate (oyster shell) Masterbatch in a PP carrier. Engineered to reduce carbon footprint in mineral filled compound.Information provided by Eurostar. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
DSM Arnite® B436 SE PBT-GF30 FR(17) 30% Glass Reinforced, Flame Retardant |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | |
A. Schulman ComAlloy Hiloy® 442 Glass Reinforced, PET Alloy Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | |
A. Schulman ComAlloy Hiloy® 617 Nylon 6, Glass/Mineral Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.55% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
Beijing Chemical Industry KAIFA® S-114 PPS Resin Glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
Bulk Molding Compounds BMC 665 Mineral Filled, Glass Reinforced Polyester BMC 665 molding compound is a mineral filled, glass reinforced polyester molding compound suitable for compression, transfer or stuffer injection molding. It is characterized by good moldability, o.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON UV00AS PPA LNP* VERTON* UV00AS is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: Heat Stabilized, Structural. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183/A |
Solvay TECHNYL® A 31T1 MZ40 PA66, 40% mineral fiber, Conditioned Description: Flame retardant polyamide PA66, 40% mineral filled, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: This.. |
|||
Density | 1.67 g/cc | 0.0603 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® SK695FR BK507 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b.. |