Material Notes:
Description: Flame retardant polyamide PA66, 40% mineral filled, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: This flame retardant material offers very good dimensional stability and excellent Glow wire performance. This product is particularly recommended for electrical parts such as: low voltage distribution, protection systems, mini circuit breakers, fuse holders and terminal blocks. This product is available in grey.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.67 g/cc
0.0603 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 47.0 MPa
6820 psi
ISO 527 Type 1A
Elongation at Break 6.9 %
6.9 %
ISO 527 Type 1A
Tensile Modulus 0.400 GPa
58.0 ksi
ISO 527 Type 1A
Electrical Properties Metric English Comments
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Users viewing this material also viewed the following: