Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 2.21 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.21 g/cc
0.0798 lb/in³
ASTM D4894
3M Dyneon™ TF 4103 PTFE 15% Glass Fiber Filled  (discontinued **)
Type II PTFE. Applications include valve seats, bearings, seals/gaskets, moldings, piston rings.Data provided by Dyneon.
Density 2.21 g/cc
0.0798 lb/in³
ASTM D792
Manifattura Cattaneo PTFE Polytetrafluoroethylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Density 2.21 g/cc
0.0798 lb/in³
ASTM 1457-62 T
Fluorseals PTFE 15% glass filled
Improved compressive strength and wear resistance.Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.
Density 2.21 g/cc

@Temperature 20.0 °C
0.0798 lb/in³

@Temperature 68.0 °F
Mateck Fused Silica IR Grade (SiO2)
Optical crystals
Density 2.21 g/cc

@Temperature 20.0 °C
0.0798 lb/in³

@Temperature 68.0 °F
Mateck Fused Silica UV-VIS Grade (SiO2)
Optical crystals
Density 2.21 g/cc
0.0798 lb/in³
Momentive Performance Materials Type 219 Fused Quartz Tubing
Known as "Ozone-Free" or "Germicidal" quartz tubing. Transmits UV-A and UV-B while blocking the deep, high energy wavelengths that cause ozone generation and pose the greatest exposure risks. Tran..
Density 2.21 g/cc
0.0798 lb/in³
Momentive Performance Materials Type 254 Fused Quartz Tubing
A doped quartz material that blocks virtually all UV-B and UV-C radiation. Ideal for lamps requiring maximum visible transmittance with nearly complete UV protection. Including some quartz halogen ..
Density 2.21 g/cc
0.0798 lb/in³
Saint-Gobain HS Grade Optical Fused Quartz
HS Grade Optical Fused Quartz is a high purity, low [OH] natural fused quartz. It has excellent IR transmission, useful transmission from 260 to 3500 nm, excellent visual quality with low bubbles, ..
Density 2.21 g/cc
0.0798 lb/in³
Saint-Gobain Spectrosil® 1000 Optical Fused Quartz
Spectrosil® 1000 grade is used for non-transmissive mirrors and substrates, and other high purity components which do not require specified optical transmission.Spectrosil® is a synthetic fuse..
Density 2.21 g/cc
0.0798 lb/in³
Saint-Gobain Spectrosil® 2000 Optical Fused Quartz
Spectrosil® 2000 is a deep UV, fluorescence-free grade.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually chlor..
Density 2.21 g/cc
0.0798 lb/in³
Saint-Gobain Spectrosil® 2100 Optical Fused Quartz
Spectrosil® 2100 has improved refractive index homogeneity.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually c..
Density 2.21 g/cc
0.0798 lb/in³
Saint-Gobain Spectrosil® 2200 Optical Fused Quartz
Spectrosil® 2200 grade is an excimer laser grade developed for maximum transmission and prolonged life in microlithography and other critical deep UV applications using KrF (248 nm) and ArF (193 ..
Density 2.21 g/cc
0.0798 lb/in³
Saint-Gobain Vitreosil® 055 Optical Fused Quartz
Vitreosil® 055 is the highest grade of optical grade fused quartz available from Saint-Gobain Quartz for use in the near UV and visible. It has a useful transmission range from 270 nm in the nea..
Density 2.21 g/cc
0.0798 lb/in³
Saint-Gobain Vitreosil® 065 066 Optical Fused Quartz
Vitreosil® 065, for use in the near UV and visible, has a less rigorous bubble specification. It has a useful transmission range from 270 nm in the near UV to 2000 nm in the IR.Vitreosil® opt..
Density 2.21 g/cc
0.0798 lb/in³
Saint-Gobain Vitreosil® Clear Fused Quartz Tubing
Electrically fused quartz is recognized for its combination of purity, chemical inertness, physical stability, thermal shock resistance, high electrical resistivity, and high operating temperatures...
Density 2.21 g/cc
0.0798 lb/in³
Saint-Gobain Puropsil® B Infrared Grade Low [OH] Optical Fused Quartz
Puropsil® B optical infrared fused quartz is manufactured from naturally occurring quartz crystal using a plasma process to ensure a low OH. It has excellent IR transmission with a useful IR tra..
Density 2.21 g/cc
0.0798 lb/in³
Corning Vycor® 7921 UV-Blocking Neodymium Blue Glass
Absorbs yellow and UV wavelengths through a process that introduces neodymium and cerium to the glass. Because the elements that create higher color temperature and UV blocking are a art of the gla..
Density 2.21 g/cc
0.0798 lb/in³
ISO 1183
Azoty Tarnow™ TARFLEN SM-S15 PTFE
15% glass fiber reinforced for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Density 2.21 g/cc
0.0798 lb/in³
ISO 1183
Azoty Tarnow™ TARFLEN SM-S15G2 PTFE