Material Notes:
Tarflen SM1 reinforced with 15% glass fibers and 2% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Physical Properties Metric English Comments
Density 2.21 g/cc
0.0798 lb/in³
ISO 1183
Particle Size 40 µm
40 µm
Average
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
ISO 868
Ball Indentation Hardness 39.0 MPa
5660 psi
ISO 2039-1
Tensile Strength, Yield 17.0 MPa
2470 psi
ISO 527
Elongation at Break 260 %
260 %
ISO 527
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ISO 180
Thermal Properties Metric English Comments
CTE, linear 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ASTM E 831
Melting Point 327 °C
621 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
IEC 60093
Surface Resistance 2.00e+13 ohm
2.00e+13 ohm
IEC 60093
Dielectric Constant 7.0
7.0
IEC 60250
Dielectric Strength 7.00 kV/mm
178 kV/in
IEC 60243-1
Dissipation Factor 0.30
0.30
IEC 60250
Processing Properties Metric English Comments
Processing Temperature 370 °C
698 °F
Molding
Back Pressure 35.0 - 40.0 MPa
5080 - 5800 psi
Molding Pressure