Indium Corp. Indalloy 176 Zinc Solder Alloy

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Zinc Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 176 Zinc Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 6.60 g/cc
0.238 lb/in³
Thermal Properties Metric English Comments
Melting Point 382 °C
720 °F
Eutectic
Solidus 382 °C
720 °F
Liquidus 382 °C
720 °F
Component Elements Properties Metric English Comments
Aluminum, Al 5.0 %
5.0 %
Zinc, Zn 95 %
95 %