Physical Properties Metric English Comments
Density 7.82 g/cc
0.283 lb/in³
Industeel URANUS® 52N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
Description: URANUS® 52N+ (UR 52N+) is a super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to re..
Density 7.82 g/cc
0.283 lb/in³
Industeel URANUS® 47N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
Description: CLI - SAF 2507® is a 25.07 super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to red..
Density 7.82 g/cc
0.283 lb/in³
Bohler-Uddeholm BÖHLER M261 Extra Plastic Lens Mold Steel
VACUUM ARC REMELTED HARDENED AND TEMPERED PLASTIC LENS MOLD STEELBOHLER M261 follow current trends in tool and die-making:Excellent machinability coupled with higher hardnessGood dimensional stabili..
Density 7.82 g/cc
0.283 lb/in³
Bohler-Uddeholm UDDEHOLM Caldie Plastic Mold Tool Steel
Description: Uddeholm Caldie is a chromium-molybdenumvanadium alloyed tool steel.Uddeholm Caldie which is characterized by:Very good chipping and cracking resistanceGood wear resistanceHigh hardness..
Density 7.82 g/cc
0.283 lb/in³
Carlson 2205 (UNS S31803) Duplex Stainless Steel
General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist..
Density 7.82 g/cc
0.283 lb/in³
Carlson 2205 (UNS S32205) Duplex Stainless Steel
General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist..
Density 7.82 g/cc
0.283 lb/in³
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 1150
AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base..
Density 7.82 g/cc
0.283 lb/in³
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150 (Heated 621°C)
Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio..
Density 7.82 g/cc
0.283 lb/in³
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150M (Heated 760°C/2hr/AC then 621°C/4hr/AC)
Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio..
Density 7.82 g/cc
0.283 lb/in³
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 1150
AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, ..
Density 7.82 g/cc
0.283 lb/in³
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 1150-M
AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, ..
Density 7.82 g/cc
0.283 lb/in³
CeramTec Sonox® P51 Piezoceramic
Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics ..