Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.91 g/cc | 0.322 lb/in³ | |
Materion ToughMet® T2 CX 90 ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
Special Metals Electroformed Nickel, 13 Micron (0.5 mil) Foil, Electroformed and Annealed Data provided by the manufacturer, Special Metals. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
Special Metals Electroformed Nickel, 200 Micron (8 mil) Foil, Electroformed and Annealed Data provided by the manufacturer, Special Metals. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
Special Metals Electroformed Nickel, 6 Micron (0.24 mil) Foil, As-Electroformed Data provided by the manufacturer, Special Metals. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
Special Metals INCONEL® alloy N06230 Ni-Cr-W-Mo Alloy INCONEL® alloy N06230 (UNS N06230 / W.Nr. 2.4733) is a carbide strengthened nickel-chromium-tungsten-molybdenum alloy with an exceptional combination of strength, stability, and resistance to cor.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | Annealed |
Eagle Brass 110 EPT COPPER, 1/2 Hard Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | Annealed |
Eagle Brass 110 EPT COPPER, 1/4 Hard Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | Annealed |
Eagle Brass 110 EPT COPPER, Hard Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | Annealed |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, 3/4 Hard 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | Annealed |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Extra Hard 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | Annealed |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Hard 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | Annealed |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Spring 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | Annealed |
Eagle Brass 194 HSM® Copper, 1/2 Hard High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | Annealed |
Eagle Brass 194 HSM® Copper, Extra Hard High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | Annealed |
Eagle Brass 194 HSM® Copper, Extra Spring High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | Annealed |
Eagle Brass 194 HSM® Copper, Spring High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
Chicago Extruded Metals BioBrass® UNS C64700 Copper-Silicon Alloy Finished product available as bar, wire, or rod.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Meta.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP4 H13 3/4 hard, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP4 H14 4/4 hard, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP4 H15 Spring, Rolled Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP4 0 Annealed, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP4 0 Annealed, Rolled Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP4 H12 1/2 hard, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP4 H12 1/2 hard, Rolled Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
Cadi C11000 ETP Standard Grade Copper The standard grade of copper - most widely used electrical conductor - suitable where mechanical design is not an issue and maximization of electrical or thermal conductivity is the primary concern... |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
California Fine Wire Nickel 220 Super Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
California Fine Wire Nickel A 200 Nickel Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
California Fine Wire Nico Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.91 g/cc | 0.322 lb/in³ | |
Schmolz + Bickenbach MoldMAX XL® Copper Alloy Description: Brush Wellman’s MoldMAX XL® is a high strength copper mold alloy with good thermal conductivity. The alloy contains no beryllium and is available in sections as large as 12” thick. .. |