Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0071 cm/cm

@Time 86400 sec
0.0071 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP KONDUIT OTF2B PPS - Linear
LNP KONDUIT* OTF2B is a compound based on PPS - Linear resin containing 10% Glass Fiber, 55% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Linear Mold Shrinkage, Transverse 0.0071 cm/cm

@Time 86400 sec
0.0071 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC
LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing 10% PTFE and 10% Aramid Fiber. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0071 cm/cm

@Time 86400 sec
0.0071 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC (Asia Pacific)
LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0071 cm/cm

@Time 86400 sec
0.0071 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DBP32EI PC
LNP* Lubricomp* DBP32EI is a compound based on Polycarbonate resin containing 15% PTFE/Silicone and 10% Glass Bead. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0071 cm/cm

@Time 86400 sec
0.0071 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DBP32EI PC (Asia Pacific)
LNP* Lubricomp* DBP32EI is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0071 cm/cm

@Time 86400 sec
0.0071 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC
LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractible, Easy Moldi..
Linear Mold Shrinkage, Transverse 0.0071 cm/cm

@Time 86400 sec
0.0071 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DFL36XXJ PC
LNP* Lubricomp* DFL36XXJ is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable, Healthcare..
Linear Mold Shrinkage, Transverse 0.0071 cm/cm

@Time 86400 sec
0.0071 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC (Asia Pacific)
LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
Linear Mold Shrinkage, Transverse 0.0071 cm/cm

@Time 86400 sec
0.0071 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp EB004 PEI
LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Transverse 0.0071 cm/cm

@Time 86400 sec
0.0071 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp EB004 PEI (Asia Pacific)
LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Asia Pacific region.
Linear Mold Shrinkage, Transverse 0.0071 cm/cm

@Time 86400 sec
0.0071 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC
LNP* THERMOCOMP* DB0049F is a compound based on Polycarbonate resin containing 20% Glass Bead. Added features of this material include: Flame Retardant, Superior Molding.
Linear Mold Shrinkage, Transverse 0.0071 cm/cm

@Time 86400 sec
0.0071 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC (Asia Pacific)
LNP* Thermocomp* DB0049F is a compound based on Polycarbonate resin containing Glass Bead, Flame Retardant. Added features of this material include: Flame Retardant, Superior Molding.