Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Bulk Density = 0.0208 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.577 - 0.705 g/cc
0.0208 - 0.0255 lb/in³
Loose
KaMin KaMin® 80B Kaolin Clay - Waterwashed
KaMin® 80B is an economical, general purpose water-washed kaolin, with intermediate brightness. It is suitable for use in water-borne, solvent-borne and solvent-free paint, ink, and adhesive appl..
Bulk Density 0.577 - 0.705 g/cc
0.0208 - 0.0255 lb/in³
Loose
KaMin Polyfil® XB Kaolin Clay - Waterwashed
Cost effective, kaolin extender offering improved consistency vs air floated clays, spray-dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, EPDM, Wire & CableIn..
Bulk Density 0.577 g/cc
0.0208 lb/in³
Dry
Skamol Group Moler HIPOROS Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Bulk Density 0.577 g/cc
0.0208 lb/in³
As Supplied
Skamol Group VERMICAST 14-100 Insulating Castable
SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f..
Bulk Density 0.577 g/cc
0.0208 lb/in³
DuPont Elvaloy® 4170 Reactive Ethylene Terpolymer (RET)
A reactive ethylene terpolymer (RET) that can be used to modify the properties of asphalt binder used in paving.Elvoy® 4170 is the most chemically reactive of the terpolymers manufactured by DuPont..
Bulk Density 0.577 g/cc
0.0208 lb/in³
Loose
CIMBAR RiverCal™ 8107 & 8107C Calcium Carbonate (CaCO3)
RiverCal™ 8100 Series Calcium Carbonate are high purity, white, functional fillers targeted for use in thermosets, thermoplastics, paint & coatings, sealants, TPO's and TPE's and other applications..