Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.577 - 0.705 g/cc | 0.0208 - 0.0255 lb/in³ | Loose |
KaMin KaMin® 80B Kaolin Clay - Waterwashed KaMin® 80B is an economical, general purpose water-washed kaolin, with intermediate brightness. It is suitable for use in water-borne, solvent-borne and solvent-free paint, ink, and adhesive appl.. |
|||
Bulk Density | 0.577 - 0.705 g/cc | 0.0208 - 0.0255 lb/in³ | Loose |
KaMin Polyfil® XB Kaolin Clay - Waterwashed Cost effective, kaolin extender offering improved consistency vs air floated clays, spray-dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, EPDM, Wire & CableIn.. |
|||
Bulk Density | 0.577 g/cc | 0.0208 lb/in³ | Dry |
Skamol Group Moler HIPOROS Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Bulk Density | 0.577 g/cc | 0.0208 lb/in³ | As Supplied |
Skamol Group VERMICAST 14-100 Insulating Castable SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f.. |
|||
Bulk Density | 0.577 g/cc | 0.0208 lb/in³ | |
DuPont Elvaloy® 4170 Reactive Ethylene Terpolymer (RET) A reactive ethylene terpolymer (RET) that can be used to modify the properties of asphalt binder used in paving.Elvoy® 4170 is the most chemically reactive of the terpolymers manufactured by DuPont.. |
|||
Bulk Density | 0.577 g/cc | 0.0208 lb/in³ | Loose |
CIMBAR RiverCal™ 8107 & 8107C Calcium Carbonate (CaCO3) RiverCal™ 8100 Series Calcium Carbonate are high purity, white, functional fillers targeted for use in thermosets, thermoplastics, paint & coatings, sealants, TPO's and TPE's and other applications.. |