Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.577 - 0.705 g/cc | 0.0208 - 0.0255 lb/in³ | Loose |
KaMin KaMin® 80B Kaolin Clay - Waterwashed KaMin® 80B is an economical, general purpose water-washed kaolin, with intermediate brightness. It is suitable for use in water-borne, solvent-borne and solvent-free paint, ink, and adhesive appl.. |
|||
Bulk Density | 0.577 - 0.705 g/cc | 0.0208 - 0.0255 lb/in³ | Loose |
KaMin Polyfil® XB Kaolin Clay - Waterwashed Cost effective, kaolin extender offering improved consistency vs air floated clays, spray-dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, EPDM, Wire & CableIn.. |
|||
Bulk Density | 0.641 - 0.705 g/cc | 0.0231 - 0.0255 lb/in³ | loose |
CIMBAR CAL-BEN™ Calcium Bentonite Selectively mined calcium bentonite, specially blended and processed for general industrial use. It is tan to yellowish in color and comes in the form of a fine powder.Incorporation:Can be base exc.. |