Material Notes:
KaMin® 80B is an economical, general purpose water-washed kaolin, with intermediate brightness. It is suitable for use in water-borne, solvent-borne and solvent-free paint, ink, and adhesive applications. Industry: Paint & Coatings, Adhesives & SealantsUses: Architectural Coatings, Industrial Coatings, Flat/Matte, Satin, Water BasedInformation provided by KaMin LLC.
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Bulk Density 0.577 - 0.705 g/cc
0.0208 - 0.0255 lb/in³
Loose
Solids Content 69.5 - 71 %
69.5 - 71 %
Slurry
Brightness 86 - 87.5 %
86 - 87.5 %
Reflectance (TAPPI)
Oil Absorption 42 %
42 %
Fineness >= 5
>= 5
Hegman Grind
Moisture Absorption at Equilibrium <= 1.5 %
<= 1.5 %
As Produced
Particle Size 0.500 µm
0.500 µm
Average Stokes Equivalent Diameter
2.30 µm
2.30 µm
Median (Malvern Laser)
Particle Mesh Size 325 Mesh
325 Mesh
0.005% Retained
pH 6 - 8
6 - 8
100 g/250 ml H2O Slurry
Specific Surface Area 17.0 m²/g
17.0 m²/g
BET
Brookfield Viscosity 450 cP

@Temperature 25.0 °C
450 cP

@Temperature 77.0 °F
20 RPM
Descriptive Properties Value Comments
Bulking Value 21.7 lb.gal
CAS Number 1332-58-7
Crystalline Silica (quartz) <0.1%
Physical Forms Dry, Slurry
Shipping Point Macon, GA