Plenco 7556 Phenolic, Briquette, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Glass Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 7556 Phenolic, Briquette, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component file E40654.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.830 g/cc
0.0300 lb/in³
ASTM D1895
Density 1.83 g/cc
0.0661 lb/in³
ASTM D792
Water Absorption 0.056 %
0.056 %
ASTM D570
Linear Mold Shrinkage 0.00094 cm/cm
0.00094 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 95
95
ASTM D785
Tensile Strength, Ultimate 76.0 MPa
11000 psi
ASTM D638
Elongation at Break 0.67 %
0.67 %
ASTM D638
Tensile Modulus 15.9 GPa
2310 ksi
ASTM D638
Flexural Strength 139 MPa
20200 psi
ASTM D790
Flexural Modulus 15.9 GPa
2310 ksi
ASTM D790
Compressive Strength 226 MPa
32800 psi
ASTM D695
Izod Impact, Notched 0.330 J/cm
0.618 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.310 J/cm²
1.48 ft-lb/in²
ASTM D256
Impact 203
203
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Thermal Conductivity 0.540 W/m-K

@Temperature 100 °C
3.75 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 217 °C
423 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 254 °C
489 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
Oxygen Index 39 %
39 %
ASTM D2863
Shrinkage 0.049 %
0.049 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 5.10e+11 ohm-cm
5.10e+11 ohm-cm
ASTM D247
Dielectric Constant 6.7
6.7
ASTM D150
Dielectric Strength 8.10 kV/mm
206 kV/in
Short Time; ASTM D149
Dissipation Factor 0.042
0.042
ASTM D150
Arc Resistance 153 sec
153 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638