Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.90 g/cc | 0.0686 lb/in³ | |
MarkeTech Repton EXP 36 Cordierite Mullite REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Bulk Density | 1.90 - 2.00 g/cc | 0.0686 - 0.0723 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 110 C Dense Refractory Castable Description: Curon 110 C is a coarse castable. Application: covers for anode baking furnaces.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Bulk Density | 1.90 - 2.00 g/cc | 0.0686 - 0.0723 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 120 C Dense Refractory Castable Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 C has good thermal shock resistance.Remarks: These values apply to cast products.Informat.. |
|||
Bulk Density | 1.90 - 2.00 g/cc | 0.0686 - 0.0723 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 120 Dense Refractory Castable Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 has good thermal shock resistance.Remarks: These values apply to cast products. Also avai.. |
|||
Bulk Density | 1.90 - 2.00 g/cc | 0.0686 - 0.0723 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 120 HS Dense Refractory Castable Description: This castable has a very good resistance against thermal shocks because of its low thermal expansion. In addition, it has a high strength. Used in incinerators and for tunnel kiln cars... |
|||
Bulk Density | 1.90 - 2.00 g/cc | 0.0686 - 0.0723 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 130 HRC Dense Refractory Castable Description: A coarse, low iron castable for use up to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRC has a good thermal shock resistance becaus.. |
|||
Bulk Density | >= 1.90 g/cc | >= 0.0686 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics ZAP 009 Smart Cast Application Special Properties: Thermal Shock, Lesser Dross Formation, Non-wetting To AluminumIndustry: Non-FerrousApplication: Aluminum Melting/Holding Furnace, Launders, Risers, Transfer LaddlesInformation pr.. |
|||
Bulk Density | 1.90 g/cc | 0.0686 lb/in³ | |
Elkem LC FeSi 65 Low Carbon Ferrosilicon This product is added as a deoxidant and as an alloying element to steels that require a special low carbon content, e.g. non-grain oriented electrical steels. Low Carbon FeSi 65 lowers the electric.. |
|||
Bulk Density | 1.90 g/cc | 0.0686 lb/in³ | |
Elkem ULC FeSi 65 Low Carbon Ferrosilicon This product is added as a deoxidant and as an alloying element to steels that require a special low carbon content, e.g. non-grain oriented electrical steels. Low Carbon FeSi 65 lowers the electric.. |
|||
Bulk Density | >= 1.90 g/cc | >= 0.0686 lb/in³ | |
China-Yixing Longly Refractories ASM-120 Cordierite-Mullite Featured mullite, cordierite as the main raw material, the use of advanced production technology, professionally manufacturing the kiln furniture of ceramic and powder metallurgy with load bearing b.. |
|||
Bulk Density | 1.90 g/cc | 0.0686 lb/in³ | |
Chosun Refractories CAR-1 Carbon Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |