Physical Properties Metric English Comments
Bulk Density 0.800 - 1.00 g/cc
0.0289 - 0.0361 lb/in³
Nabaltec NABALOX® NO 105 Calcined Aluminum Oxide
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Bulk Density 0.800 - 1.00 g/cc
0.0289 - 0.0361 lb/in³
Nabaltec NABALOX® NO 105 RA Calcined Aluminum Oxide
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Bulk Density 0.800 - 1.00 g/cc
0.0289 - 0.0361 lb/in³
Nabaltec NABALOX® NO 201 Calcined Aluminum Oxide
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Bulk Density 0.800 - 1.00 g/cc
0.0289 - 0.0361 lb/in³
Nabaltec NABALOX® NO 713-10 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Bulk Density 0.800 - 1.00 g/cc
0.0289 - 0.0361 lb/in³
Nabaltec NABALOX® NO 713-40 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Bulk Density 0.800 - 1.00 g/cc
0.0289 - 0.0361 lb/in³
Nabaltec NABALOX® NO 715-10 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Bulk Density 0.800 - 1.00 g/cc
0.0289 - 0.0361 lb/in³
Nabaltec NABALOX® NO 725-10 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Bulk Density 0.700 - 1.00 g/cc
0.0253 - 0.0361 lb/in³
Magyar Aluminum ALO-DFM Alumina
Alumina for Polishing
Bulk Density 0.600 - 1.00 g/cc
0.0217 - 0.0361 lb/in³
tapped
Solvay Chemicals Barium carbonate fine powder
Barium carbonate fine powder is specially developed for usage in the brick and tile industry and for the removing of sulfates. Other applications are in the ceramic and ferrite industry. It is also ..