Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.50 - 2.60 g/cc | 0.0903 - 0.0939 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS SiC 90 D Moldable Refractory Material Description: This material is supplied as a dry powder. It has to be mixed with clean water to the necessary consistency. Curas SiC 90 has a phosphate bond and especially meant for protection of bo.. |
|||
Bulk Density | 2.50 - 2.60 g/cc | 0.0903 - 0.0939 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 160 C Dense Refractory Castable Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 C has an excellent thermal shoc.. |
|||
Bulk Density | 2.50 - 2.60 g/cc | 0.0903 - 0.0939 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 120 S Dense Refractory Castable Description: A very strong castable with a high abrasion resistance of which both aggregate and cement attribute to hydraulic binding.Remarks: These values apply to cast products. Also available in .. |
|||
Bulk Density | 2.50 - 2.60 g/cc | 0.0903 - 0.0939 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 13 S Dense Refractory Castable Description: Curon 13 S is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/hol.. |
|||
Bulk Density | 2.50 - 2.60 g/cc | 0.0903 - 0.0939 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 13 SC Dense Refractory Castable Description: Curon 13 SC is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/ho.. |
|||
Bulk Density | 2.50 - 2.60 g/cc | 0.0903 - 0.0939 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 14 S Dense Refractory Castable Description: Curon 14 S is a dense, strong and abrasion resistant castable. Because of the very low percentage of Fe2O3 and SiO2 it is used for highly abrasive conditions in reducing atmospheres.Rem.. |
|||
Bulk Density | 2.50 - 2.60 g/cc | 0.0903 - 0.0939 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 150 Dense Refractory Castable Description: This bauxite based castable has a very good thermal shock resistance and is therefore well suited for burner blocks.Remarks: These values apply to cast products. Also available in gunni.. |
|||
Bulk Density | 2.50 - 2.60 g/cc | 0.0903 - 0.0939 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 160 H RAPID Dense Vibrating Refractory Castable Description: Vibron 160 H Rap is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance. Because of special additives, thi.. |
|||
Bulk Density | 2.50 - 2.60 g/cc | 0.0903 - 0.0939 lb/in³ | |
Chosun Refractories CUN-669 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.50 - 2.60 g/cc | 0.0903 - 0.0939 lb/in³ | After drying at 110°C |
Gouda Vuurvast FLUCON 160 H Dense Self Flowing Refractory Castable Description: Flucon 160 H is a self-flowing low cement castable on high fired high alumina grog base, characterized by a high strength and good thermal shock resistance.Remarks: These values apply t.. |