Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | outside diameter |
NanoAmor 95%, OD/ID/L: 20-40/5-10 nm/1-2 um Short Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | outside diameter |
NanoAmor 95%, OD/ID: 20-40/5-10 nm Aligned Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | outside diameter |
NanoAmor 95%, OD/WT/L: 20-40/5-15 nm/0.5-5 um Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Antimony Nanoparticles General DescriptionAntimony (Sb) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Antimony Particles are typically 20-40 nano.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Antimony Tin Oxide Nanoparticles General DescriptionAntimony Tin Oxide (ATO) Nanoparticles, nanopowder, nanodots or nanocrystals are spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties. N.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Barium Titanate nanoparticles General DescriptionBarium Titanate Nanoparticles, nanopowder, nanodots or nanocrystals are spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties. Nanoscale .. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Indium Nanoparticles General DescriptionIndium (In) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Indium Particles are typically 20-40 nanomete.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Iron Cobalt Nanopowder General DescriptionIron Cobalt ( FeCo) Nanopowder or Nanoparticles, nanodots or nanocrystals are black spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Iron Nanoparticles General DescriptionIron (Fe) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Iron Particles are typically 20-40 nanometers (.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Iron Oxide Nanopowder General DescriptionIron Oxide ( Fe2O3 and Fe3O4) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure part.. |
|||
Particle Size | 0.0050 - 0.040 µm | 0.0050 - 0.040 µm | |
American Elements Lanthanum Nanoparticles General DescriptionLanthanum (La) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Lanthanum Particles are typically 5 - 40 nanometers (nm) with speci.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Lead Oxide Nanopowder General DescriptionLead Oxide ( PbO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Lead Oxide Par.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Manganese Nanoparticles General DescriptionManganese (Mn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Manganese Particles are typically 20-40 na.. |
|||
Particle Size | 0.010 - 0.040 µm | 0.010 - 0.040 µm | |
American Elements Nickel Nanoparticles General DescriptionNickel (Ni) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Nickel Particles are typically 10 - 40 nanometers (nm) with specific s.. |
|||
Particle Size | 0.010 - 0.040 µm | 0.010 - 0.040 µm | |
American Elements Nickel Titanium Nanoparticles General DescriptionNickel Titanium (NiTi) Nanoparticles, nanodots or nanopowder are black spherical high surface area alloy particles. Nanoscale Nickel Titanium Particles are typically 10 - 40 nanom.. |
|||
Particle Size | 0.0010 - 0.040 µm | 0.0010 - 0.040 µm | |
American Elements Silver Nanoparticles General DescriptionSilver (Ag) Nanoparticles, nanodots or nanopowder are spherical or flake high surface area metal particles. Nanoscale Silver Particles are typically 1 - 40 nanometers (nm) with sp.. |
|||
Particle Size | 0.0050 - 0.040 µm | 0.0050 - 0.040 µm | |
American Elements Strontium Carbonate Nanoparticles General DescriptionStrontium Carbonate (SrCO3) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Strontium Carbonate Particles are typically 5 - 40 nan.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Tin Oxide Nanopowder General DescriptionTin Oxide ( SnO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Tin Oxide Parti.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Tungsten Oxide Nanopowder General DescriptionTungsten Oxide ( WO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Tin Oxide P.. |
|||
Particle Size | 0.010 - 0.040 µm | 0.010 - 0.040 µm | |
American Elements Zirconium Nanoparticles General DescriptionZirconium (Zr) Nanoparticles, nanodots or Nanopowder are black spherical high surface area metal particles. Nanoscale Zirconium Particles are typically 10-40 nanometers (nm) with .. |
|||
Particle Size | 0.0050 - 0.040 µm | 0.0050 - 0.040 µm | |
American Elements Cerium Nanoparticles General DescriptionCerium (Ce) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Cerium Particles are typically 5 - 40 nanometers (nm) with specific su.. |
|||
Particle Size | 0.020 - 0.040 µm | 0.020 - 0.040 µm | |
American Elements Cobalt Iron Nanopowder General DescriptionCobalt Iron ( CoFe) Nanopowder or Nanoparticles, nanodots or nanocrystals are black spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties.. |