Polymer Property : Particle Size = 0.045 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 0.010 - 0.045 µm
0.010 - 0.045 µm
American Elements Europium Nanoparticles
General DescriptionEuropium (Eu) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Europium Particles are typically 10 - 45 nanometers (nm) with specif..
Particle Size 0.010 - 0.045 µm
0.010 - 0.045 µm
American Elements Gadolinium Nanoparticles
General DescriptionGadolinium (Gd) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Gadolinium Particles are typically 10 - 45 nanometers (nm) with sp..
Particle Size 0.010 - 0.045 µm
0.010 - 0.045 µm
American Elements Neodymium Nanoparticles
General DescriptionNeodymium (Nd) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Neodymium Particles are typically 10 - 45 nanometers (nm) with spec..
Particle Size 0.010 - 0.045 µm
0.010 - 0.045 µm
American Elements Praseodymium Nanoparticles
General DescriptionPraseodymium (Pr) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Praseodymium Particles are typically 10 - 45 nanometers (nm) wit..
Particle Size 0.0050 - 0.045 µm
0.0050 - 0.045 µm
American Elements Yttrium Nanoparticles
General DescriptionYttrium (Y) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Yttrium Particles are typically 5 - 45 nanometers (nm) with specific s..
Particle Size 0.010 - 0.045 µm
0.010 - 0.045 µm
American Elements Carbon Nanoparticles
General DescriptionCarbon (C) Nanoparticles, nanodots or nanopowder are black spherical high surface area graphitic carbon. Nanoscale Carbon Particles are typically 10 - 45 nanometers (nm) with spec..