Physical Properties Metric English Comments
Particle Size 0.050 - 0.080 µm
0.050 - 0.080 µm
outside diameter
NanoAmor 95%, OD/ID/L: 50-80/5-15 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size 0.050 - 0.080 µm
0.050 - 0.080 µm
outside diameter
NanoAmor 95%, OD: 50-80 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size 0.050 - 0.080 µm
0.050 - 0.080 µm
outside diameter
NanoAmor 95%, OD: 50-80 nm OH Functionalized Aligned Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size 0.050 - 0.080 µm
0.050 - 0.080 µm
outside diameter
NanoAmor 95%, OD/ID: 50-80/5-15 nm Aligned Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size <= 0.050 µm
<= 0.050 µm
D<sub>50</sub>
Heraeus Cleviosâ„¢ P VP CH 8000 Conductive Sulfonate Polymer for Antistatic Coatings
Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P VP CH 8000 is an antistatic material based o..
Particle Size 0.050 - 0.10 µm
0.050 - 0.10 µm
American Elements Molybdenum Nanoparticles
General DescriptionMolybdenum (Mo) Nanoparticles, nanodots or nanopowder are black high surface area particles. Nanoscale Molybdenum Particles are typically 50 - 100 nanometers (nm) with specific su..
Particle Size 0.050 - 0.10 µm
0.050 - 0.10 µm
American Elements Nickel Nanoparticles
General DescriptionNickel (Ni) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Nickel Particles are typically 10 - 40 nanometers (nm) with specific s..
Particle Size 0.050 - 0.10 µm
0.050 - 0.10 µm
American Elements Nickel Titanium Nanoparticles
General DescriptionNickel Titanium (NiTi) Nanoparticles, nanodots or nanopowder are black spherical high surface area alloy particles. Nanoscale Nickel Titanium Particles are typically 10 - 40 nanom..
Particle Size 0.050 - 0.10 µm
0.050 - 0.10 µm
American Elements Zirconium Nanoparticles
General DescriptionZirconium (Zr) Nanoparticles, nanodots or Nanopowder are black spherical high surface area metal particles. Nanoscale Zirconium Particles are typically 10-40 nanometers (nm) with ..