Physical Properties Metric English Comments
Particle Size 0.050 - 0.080 µm
0.050 - 0.080 µm
outside diameter
NanoAmor 95%, OD/ID/L: 50-80/5-15 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size 0.050 - 0.080 µm
0.050 - 0.080 µm
outside diameter
NanoAmor 95%, OD: 50-80 nm COOH Functionalized Aligned Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size 0.050 - 0.080 µm
0.050 - 0.080 µm
outside diameter
NanoAmor 95%, OD: 50-80 nm OH Functionalized Aligned Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size 0.050 - 0.080 µm
0.050 - 0.080 µm
outside diameter
NanoAmor 95%, OD/ID: 50-80/5-15 nm Aligned Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Particle Size 0.020 - 0.080 µm
0.020 - 0.080 µm
American Elements Antimony Oxide Nanopowder
General DescriptionAntimony Oxide ( SbO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. N..
Particle Size 0.020 - 0.080 µm
0.020 - 0.080 µm
American Elements Bismuth Oxide Nanopowder
General DescriptionBismuth Oxide ( BiO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Na..
Particle Size 0.010 - 0.080 µm
0.010 - 0.080 µm
American Elements Calcium Carbonate Nanoparticles
General DescriptionCalcium Carbonate (CaCO3) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Calcium Carbonate Particles are typically 10 - 80 nanometers (..
Particle Size 0.010 - 0.080 µm
0.010 - 0.080 µm
American Elements Dysprosium Nanoparticles
General DescriptionDysprosium (Dy) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Particles are typically 10 - 80 nanometers (nm) with sp..
Particle Size 0.010 - 0.080 µm
0.010 - 0.080 µm
American Elements Dysprosium Oxide Nanopowder
General DescriptionDysprosium (DyO) Oxide Nanopowder or Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Oxide Particles are typically 10 -..
Particle Size 0.010 - 0.080 µm
0.010 - 0.080 µm
American Elements Erbium Nanoparticles
General DescriptionErbium (Er) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Erbium Particles are typically 10 - 80 nanometers (nm) with specific s..
Particle Size 0.030 - 0.080 µm
0.030 - 0.080 µm
American Elements Holmium Nanoparticles
General DescriptionHolmium (Ho) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Dysprosium Particles are typically 30 - 80 nanometers (nm) with speci..
Particle Size 0.020 - 0.080 µm
0.020 - 0.080 µm
American Elements Molybdenum Oxide Nanopowder
General DescriptionMolybdenum Oxide ( MoO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles...
Particle Size 0.020 - 0.080 µm
0.020 - 0.080 µm
American Elements Tantalum Oxide Nanopowder
General DescriptionTantalum Oxide ( TaO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. N..
Particle Size 0.010 - 0.080 µm
0.010 - 0.080 µm
American Elements Terbium Nanoparticles
General DescriptionTerbium (Tb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Terbium Particles are typically 10 - 80 nanometers (nm) with specific..
Particle Size 0.010 - 0.080 µm
0.010 - 0.080 µm
American Elements Titanium Nanoparticles
General DescriptionTitanium (Ti) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Titanium Particles are typically 10 - 80 nanometers (nm) ..
Particle Size 0.040 - 0.080 µm
0.040 - 0.080 µm
American Elements Tungsten Nanoparticles
General DescriptionTungsten (W) Nanoparticles, nanodots or nanopowder are black spherical high surface area metal particles. Nanoscale Tungsten Particles are typically 40-80 nanometers (nm) with spe..
Particle Size 0.010 - 0.080 µm
0.010 - 0.080 µm
American Elements Ytterbium Nanoparticles
General DescriptionYtterbium (Yb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Ytterbium Particles are typically 10 - 80 nanometers (nm) with spec..
Particle Size 0.020 - 0.080 µm
0.020 - 0.080 µm
American Elements Calcium Oxide Nanopowder
General DescriptionCalcium Oxide ( CaO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Na..
Particle Size 0.010 - 0.080 µm
0.010 - 0.080 µm
American Elements Calcium Phosphate Nanoparticles
General DescriptionCalcium Phosphate (CAP) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Calcium Phosphate Particles are typically 10 - 80 nanometers (nm..