Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 14 µm | 14 µm | median; Microtrac |
Nyco NYAD® 325 Wollastonite Powdered grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particl.. |
|||
Particle Size | 14 µm | 14 µm | median; Microtrac |
Nyco NYGLOS® STPO Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Particle Size | 14 µm | 14 µm | mean; 99% -325 mesh |
Momentive Performance Materials HCT-30D Titanium Diboride (TiB2) Powder Grade HCT-30D is tailored for fabrication by the hot-pressing process. Its composition provides for ease and optimizes the mechanical properties of the component shapes.Titanium Diboride Powder .. |
|||
Particle Size | 14 - 18 µm | 14 - 18 µm | 50% |
H.C. Starck Amperit® 251 Gas Atomized (NiCr 80-20) |
|||
Particle Size | 14 - 18 µm | 14 - 18 µm | 50% |
H.C. Starck Amperit® 281 Gas Atomized (NiAl 95-5) |
|||
Particle Size | 14 - 38 µm | 14 - 38 µm | d90 |
Indium Corp. In2O3 Type A Indium Oxide, Crystalline Powder Indium Sesquioxide is a yellow colored powder. It is a stable ceramic-like material, insoluble in water and volatizes at 850°C. Indium sesquioxide is a n-type semiconductor and as such is used .. |
|||
Particle Size | 14 - 19 µm | 14 - 19 µm | 10% |
H.C. Starck Amperit® 553.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr) |
|||
Particle Size | 14 - 18 µm | 14 - 18 µm | 50% |
H.C. Starck Amperit® 554.071 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr) |
|||
Particle Size | 14 µm | 14 µm | |
Silberline "A" Series A-222FG A-222FG is a fine, non-leafing aluminum pigment with good opacity for solvent based industrial coatings. This grade has a cornflake geometry and wide particle size distribution range. This grade can.. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline A-6211 A-6211 is a standard grade; class B, medium sized, leafing aluminum pigment carried in C-66 exempt mineral spirits.Applications: Trade & Maintenance |
|||
Particle Size | 14 µm | 14 µm | |
Silberline Aquasil® "BP" 5500 Silberline has specifically created Aquasil® BP grades for aqueous architectural and industrial maintenance coatings. This family offers a cost-effective alternative for achieving stability and .. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline Aquasil® "BP" SN Silberline has specifically created Aquasil® BP grades for aqueous architectural and industrial maintenance coatings. This family offers a cost-effective alternative for achieving stability and .. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline EternaBrite® 301-1 EternaBrite® pigments are leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on cornflake geometry and offer enhanced leafing properties in solvent and waterborn.. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline SilBerCote® 5588-20Y SilBerCote® Y polymer treated aluminum pigments are resistant to acid and alkali staining, while providing enhanced electrical charge resistance in finished coatings. SilBerCote® Y imparts add.. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline SilBerCote® PC 8153X SilBerCote® PC X can be formulated into post-blend and bonded metallic powder coatings. The inorganic surface treatment on the flake imparts improved chemical and environmental resistance propert.. |
|||
Particle Size | 14 µm | 14 µm | Before Conversion |
Silberline Silvet® 320-20-J Silvet® "J" pigments are leafing and non-leafing aluminum pigment pellets designed for ease of handling and incorporation in solvent borne flexographic and gravure ink formulations. The pigment p.. |
|||
Particle Size | 14 µm | 14 µm | Before Conversion |
Silberline Silvet® 960-20-P Silvet® P grades are recommended for use with engineering resins or transparent polymers where compatibility, maintenance of polymer clarity and distinctiveness of image (D.O.I.) observed from th.. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline Silvex® 223-20-C Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline Silvex® 225-20-D Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline Sparkle Silvex® 965-30-D Sparkle Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Particle Size | 14 - 16 µm | 14 - 16 µm | D50 |
Sinotek Materials ZSG-15 Spherical Graphite Also called "Potato Graphite", Spherical Graphite is ideal cathode material for lithium ion batteries. Using high quality natural flake graphite as raw material, a series of shaping, classification.. |
|||
Particle Size | 14 µm | 14 µm | 95%, Laser diffraction; QSOP-5&75 |
Shamrock Technologies Fluoro T® 611 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline "L" Series L-476 L-476 is a fine, non-leafing aluminum pigment with good opacity for solvent based industrial coatings. This grade has a cornflake geometry and wide particle size distribution range. This grade can b.. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline Aquavexâ„¢ E5000-AR-207S Aquavexâ„¢ grades are aluminum pigment pellets designed for use in aqueous inks for flexographic and gravure printing. The pellets are composed of 80% aluminum pigment and 20% of a proprietary no.. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline Sparkle Silver® 5000-AR Sparkle Silver® 5000-AR is a fine, bright, non-leafing aluminum pigment with a narrow particle size distribution. It provides exceptional brightness and is acid resistant.Applications: Automotive.. |
|||
Particle Size | 14 µm | 14 µm | |
Silberline Sparkle Silver® 5500 Sparkle Silver® 5500 is a fine, regular purity, non-leafing aluminum pigment. It is characterized by a relatively wide particle size distribution.Applications: Automotive; General Industrial |
|||
Particle Size | 14 µm | 14 µm | |
Silberline Tufflake® 4615 Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app.. |
|||
Particle Size | 14 - 20 µm | 14 - 20 µm | d90, Guaranteed |
TIMCAL TIMREX® C-LUB 306 Primary Synthetic Graphite Information provided by TIMCAL |
|||
Particle Size | 14 µm | 14 µm | median |
Esstech V-117-1140 Barium Borosilicate Glass Barium Borosilicate glass filler or BBAS has been traditionally used in the classic dental composite systems involving bisGMA and triethyleneglycol dimethacrylate. It is available in a variety of pa.. |
|||
Particle Size | 14 µm | 14 µm | Before Conversion |
Silberline Sparkle Silvet® 960-20-J Sparkle Silvet® "J" pigments are leafing and non-leafing aluminum pigment pellets designed for ease of handling and incorporation in solvent borne flexographic and gravure ink formulations. The pig.. |