Silberline Aquasil® "BP" SN

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Silberline
Trade Name Aquasil® "BP"
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silberline Aquasil® "BP" SN.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silberline has specifically created Aquasil® BP grades for aqueous architectural and industrial maintenance coatings. This family offers a cost-effective alternative for achieving stability and system compatibility with a broad range of coating vehicles. This range of aluminum pigment grades offers aesthetics to meet virtually any formulating requirement.Applications: General Industrial; Waterborne
Physical Properties Metric English Comments
Specific Gravity 1.49 g/cc
1.49 g/cc
Bulk Factor 0.080
0.080
Volatiles 37 %
37 %
Particle Size 14 µm
14 µm
Particle Mesh Size <= 325 Mesh
<= 325 Mesh
1% retained
Descriptive Properties Value Comments
Aluminum Flake, wt% 54
Category Non-leafing
Solvents Mineral Spirits/High Aromatic/Nitroethane/Propylene Glycol Ether