Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 3.0 - 4.0 µm | 3.0 - 4.0 µm | D<sub>50</sub> |
NYC YT3X Y2O3 Powder |
|||
Particle Size | 3.0 - 4.0 µm | 3.0 - 4.0 µm | Primary |
NYC YT3X Y2O3 Powder |
|||
Particle Size | 2.0 - 4.0 µm | 2.0 - 4.0 µm | d50 |
Magyar Aluminum ALOLT 59AF Aluminum Hydroxide Ground type |
|||
Particle Size | 2.0 - 4.0 µm | 2.0 - 4.0 µm | d50 |
Magyar Aluminum ALO-P95-01 Alumina Alumina for Polishing |
|||
Particle Size | 3.0 - 4.0 µm | 3.0 - 4.0 µm | Average |
Malvern Minerals Trikup® PF Silane Treated Aluminum Hydroxide Trikup® is a custom, silane treated alumina trihydrate or aluminum hydroxide. ATH is the largest volume flame retardant in the world. Trikup® adds additional functionality through the use of .. |
|||
Particle Size | 2.0 - 4.0 µm | 2.0 - 4.0 µm | Laser Diffraction D50 |
H.C. Starck Grade B Titanium Carbonitride Hard metals (tooling and machining)CermetsBlack ceramics |
|||
Particle Size | 2.0 - 4.0 µm | 2.0 - 4.0 µm | Laser Diffraction D50 |
H.C. Starck Grade B Titanium Nitride Additive for ceramic parts to increase electrical conductivityConstituent for cermets and black ceramicsRaw material for TiN sputter targets |
|||
Particle Size | 1.0 - 4.0 µm | 1.0 - 4.0 µm | Laser Diffraction D50 |
H.C. Starck Grade III Amorphous Boron Automotive (igniter in airbags and belt tighteners)Additive in pyrotechnic mixtures (flares, igniters, and delay compositions)Additive in solid rocket propellant fuels and explosivesPreparation of r.. |
|||
Particle Size | 1.5 - 4.0 µm | 1.5 - 4.0 µm | Laser Diffraction D50 |
H.C. Starck Grade D Titanium Carbonitride Narrow grain distribution and low oxygen contentHard metals (tooling and machining)CermetsBlack ceramics |
|||
Particle Size | 3.0 - 4.0 µm | 3.0 - 4.0 µm | |
Dow Corning EP-9261 TI Cosmetic Powder This cosmetic powder provides smoothness and a powdery, non-greasy skin feel; high sebum absorption; soft focus; and improves SPF. As a white cross-linked dimethyl polysiloxane elastomer powder comb.. |
|||
Particle Size | 3.0 - 4.0 µm | 3.0 - 4.0 µm | |
Dow Corning PF-2520 ELASTOMER EMULSION DOW CORNING® PF-2520 Elastomer Emulsion has been developed to facilitate the incorporation of an elastomeric powder in fluid into water-based silicone powder into water-based cosmetic products. It .. |
|||
Particle Size | 2.0 - 4.0 µm | 2.0 - 4.0 µm | D50 |
CIMBAR UltraMag & UltraMag ST 3 Magnesium Hydroxide Powder UltraMag is a naturally ground, white, high-purity Magnesium Hydroxide suitable for a wide range of applications including water treatment slurries, plastics, rubber and flame-retardant/smoke suppre.. |