Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 2.0 - 6.0 µm | 2.0 - 6.0 µm | Primary crystal size |
Magyar Aluminum ALO-Ex35 LS Alumina Calcined Alumina |
|||
Particle Size | 3.0 - 6.0 µm | 3.0 - 6.0 µm | d50 |
Magyar Aluminum ALOLT 50AF Aluminum Hydroxide Ground type |
|||
Particle Size | 3.0 - 6.0 µm | 3.0 - 6.0 µm | d50 |
Magyar Aluminum ALO-P54-04 Alumina Alumina for Polishing |
|||
Particle Size | 3.0 - 6.0 µm | 3.0 - 6.0 µm | mean; 100% -325 mesh |
Momentive Performance Materials HCT-F Titanium Diboride (TiB2) Powder Grade HCT-F powders are designed for use on applications requiring reduced particle size without sacrificing high purity.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced.. |
|||
Particle Size | 4.0 - 6.0 µm | 4.0 - 6.0 µm | 10% |
H.C. Starck Amperit® 140.067 Tungsten (W) HS Number: 81011000 |
|||
Particle Size | 3.0 - 6.0 µm | 3.0 - 6.0 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade D Titanium Diboride, TiB2 Powder for hot pressing, technical grade.Hot-pressed composites of excellent electrical conductivity, e.g., evaporation boats for continuous aluminum metallizingCrucible material for non-ferrous met.. |
|||
Particle Size | 3.0 - 6.0 µm | 3.0 - 6.0 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade SE Titanium Diboride, TiB2 Higher N, O, Fe contentsHot-pressed composites of excellent electrical conductivity, e.g., evaporation boats for continuous aluminum metallizingCrucible material for non-ferrous metalsCeramic shapes.. |
|||
Particle Size | 2.0 - 6.0 µm | 2.0 - 6.0 µm | X50% |
Solvay Chemicals NOCOLOK® Flux P2 Potassium Fluoroaluminate Mixtures of NOCOLOK® Flux P2 with NOCOLOK® Flux allow for gradual viscosity adjustments in suspensions to suit specific process conditions.HS No.: 38109090 /CAS-No.: 60304-36-1Uses: Automoti.. |
|||
Particle Size | 4.0 - 6.0 µm | 4.0 - 6.0 µm | Average; ATO 40-41-0 (Coulter Counter) |
Arkema Group ORGASOL® 2001 UD Nat 2 Polyamide 12, Food Contact Approved Information provided by Arkema Group |
|||
Particle Size | 4.0 - 6.0 µm | 4.0 - 6.0 µm | Mean particle size |
Carborundum CarboTherm™ CTUF Boron Nitride Powder Boron Nitride powders have high thermal conductivity, low dielectric loss, and low thermal expansion. They are non-abrading to electronic components, lubricious, non-toxic, and retain their dielect.. |