Polymer Property : Antiblock Level = 1800 ppm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Antiblock Level 1800 ppm
1800 ppm
SiO<sub>2</sub>; Borealis Method
Borealis BorPure™ RD226CF Polypropylene Random Copolymer
BorPure™ RD226CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: BorPure™ RD226CF is recommended for food packaging..
Antiblock Level 1800 ppm
1800 ppm
SiO<sub>2</sub>; Borealis Method
Borealis BorPure™ RD234CF Polypropylene Random Copolymer
BorPure™ RD234CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD234CF is recommended for food packaging, stationa..
Antiblock Level 1800 ppm
1800 ppm
SiO<sub>2</sub>; Borealis Method
Borealis HD234CF Polypropylene
HD234CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: HD234CF is recommended for food packaging, lamination films, stationery f..
Antiblock Level 1800 ppm
1800 ppm
SiO<sub>2</sub>; Borealis Method
Borealis HD822CF Polypropylene
HD822CF is a polypropylene homopolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: food packaging, lamination films, statio..
Antiblock Level 1800 ppm
1800 ppm
SiO<sub>2</sub>; Borealis Method
Borealis RD461CF Polypropylene Random Copolymer
RD461CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD461CF is recommended for food packaging, high quality stati..
Antiblock Level 1800 ppm
1800 ppm
SiO<sub>2</sub>; Borealis Method
Borealis RD734CF Polypropylene Random Copolymer
RD734CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD734CF is recommended for food packaging, high quality stati..
Antiblock Level 1800 ppm
1800 ppm
SiO2
Total PPH 3576 BB Polypropylene Homopolymer, Cast Film
Polypropylene 3576 BB is recommended for use in non-oriented cast films processes. It contains an optimized level of slip and anti-block additives.3576 BB is intended for food, magazine or textile ..
Antiblock Level 1800 ppm
1800 ppm
SiO2
Total PPH 6088 Polypropylene Homopolymer, Cast Film
Polypropylene PPH 6088 is a homopolymer polypropylene with a Melt Flow index of 9 g/10 min for the cast extrusion of film with excellent optical properties and good sterilizability.Polypropylene PPH..
Antiblock Level 1800 ppm
1800 ppm
SiO2
Total PPR 6288 Random Copolymer Polypropylene, Cast Extrusion of Film
Total Petrochemicals PPR 6288 is a random copolymer polypropylene with a melt flow index of 8 g/10 min for the cast extrusion of films with outstanding optical properties and easy heat weldability.P..
Antiblock Level 1800 ppm
1800 ppm
ExxonMobil LDPE LD 158JD Low Density Polyethylene Resin
Product Description: LD 158 series are LDPE grades, specially designed for lamination and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very low gel ..
Antiblock Level 1800 ppm
1800 ppm
ExxonMobil LDPE LD 185JD Low Density Polyethylene Resin (European Grade)
Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio..
Antiblock Level 1800 ppm
1800 ppm
ExxonMobil LDPE LD 361JD Low Density Polyethylene Resin
Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Antiblock Level 1800 ppm
1800 ppm
ExxonMobil LDPE LD 368HD Low Density Polyethylene Resin
Product Description: LD 368 series are high clarity EVA LDPE grades, offering good optical properties combined with toughness and impact resistance. Two additive combinations are available according..
Antiblock Level 1800 ppm
1800 ppm
SiO<sub>2</sub>; Borealis Method
Borealis HD214CF Polypropylene Homopolymer
HD214CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: food packaging, lamination films, stationary films, multi layer co-extrus..