Material Notes:
Product Description: LD 158 series are LDPE grades, specially designed for lamination and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very low gel level. These grades have a Film Appearance specification. Two additive packages are available tailored to the needs of the laminator. LD 158 is manufactured with narrow specifications to suit the high consistency requirements of lamination films. Availability: Africa & Middle East and Europe Additive: Antiblock: 1800 ppmSlip: 330 ppmThermal Stabilizer: YesApplications: Bread BagsCo-extrusion FilmsDisplay Packaging FilmFood packagingForm Fill and Seal PackagingHigh Clarity FilmHigh Quality LaminationLamination FilmInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ExxonMobil method
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 1800 ppm
1800 ppm
Slip Level 330 ppm
330 ppm
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 200 %
200 %
ASTM D882
Film Elongation at Break, TD 500 %
500 %
ASTM D882
Elmendorf Tear Strength MD 200 g
200 g
ASTM D1922
Elmendorf Tear Strength TD 120 g
120 g
ASTM D1922
Dart Drop Test 80.0 g
0.176 lb
ASTM D1709A
Film Tensile Strength at Break, MD 22.8 MPa
3300 psi
ASTM D882
Film Tensile Strength at Break, TD 20.7 MPa
3000 psi
ASTM D882
1% Secant Modulus, MD 241 MPa
35000 psi
ASTM D882
1% Secant Modulus, TD 283 MPa
41000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 232 °C
<= 450 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 5.0 %
5.0 %
ASTM D1003
Gloss 69 %
69 %
45°; ASTM D2457