Polymer Property : Linear Mold Shrinkage = 0.0265 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.000900 - 0.0265 cm/cm
0.000900 - 0.0265 in/in
Average value: 0.0120 cm/cm Grade Count:236
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..