Polymer Property : Linear Mold Shrinkage = 0.000900 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.000900 - 0.0265 cm/cm
0.000900 - 0.0265 in/in
Average value: 0.0120 cm/cm Grade Count:236
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Linear Mold Shrinkage 0.000900 - 0.0120 cm/cm
0.000900 - 0.0120 in/in
Average value: 0.00745 cm/cm Grade Count:41
Overview of materials for Polypropylene with 20% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are..
Linear Mold Shrinkage 0.000900 - 0.0600 cm/cm
0.000900 - 0.0600 in/in
Average value: 0.00964 cm/cm Grade Count:177
Overview of materials for Polypropylene, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values..