Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.000900 - 0.0265 cm/cm | 0.000900 - 0.0265 in/in | Average value: 0.0120 cm/cm Grade Count:236 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Linear Mold Shrinkage | 0.000900 - 0.0120 cm/cm | 0.000900 - 0.0120 in/in | Average value: 0.00745 cm/cm Grade Count:41 |
Overview of materials for Polypropylene with 20% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are.. |
|||
Linear Mold Shrinkage | 0.000900 - 0.0600 cm/cm | 0.000900 - 0.0600 in/in | Average value: 0.00964 cm/cm Grade Count:177 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |