Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.00060 - 0.00090 cm/cm | 0.00060 - 0.00090 in/in | ASTM D955 and ISO 294-4 |
Ravago Manufacturing Americas Hylon® N1213HL BK Nylon 6/6 Available in North America Filler: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantForm: Pellets Proces.. |
|||
Linear Mold Shrinkage, Flow | 0.00060 cm/cm | 0.00060 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Durethan® AKV 35 HR H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.00060 cm/cm | 0.00060 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4 |
Lanxess Durethan® BKV 130 GIT DUS008 900116 Nylon 6, Impact Modified PA 6, 30% glass fibers, injection molding, impact modified, GIT/WITInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.00060 - 0.00080 cm/cm @Time 86400 sec |
0.00060 - 0.00080 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP QCL34 PA6.10 LNP* LUBRICOMP* QCL34 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.00060 - 0.00090 cm/cm @Time 86400 sec |
0.00060 - 0.00090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP UX06427 PPA LNP* LUBRICOMP* UX06427 is a compound based on PPA containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Heat Stabilized, Hot Water Moldable, Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.00060 cm/cm | 0.00060 in/in | ISO 294-4 |
Solvay Specialty Polymers Kalix® 5950 HFFR Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 5950 HFFR is a halogen-free, flame retardant (UL-94 V0 at 0.4 mm), highly reinforced polyamide material specifically formulated for high strength and stiffness applications where good impa.. |
|||
Linear Mold Shrinkage, Flow | 0.00060 - 0.00090 cm/cm @Time 86400 sec |
0.00060 - 0.00090 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DE004ER PC LNP* STAT-KON* DE004ER is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added featuresof this material include: Electrically Conductive, Easy Molding, Mold Release. |
|||
Linear Mold Shrinkage, Flow | 0.00060 - 0.00080 cm/cm @Time 86400 sec |
0.00060 - 0.00080 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DEF42 PC LNP STAT-KON* DEF42 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.00060 cm/cm @Time 86400 sec |
0.00060 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON DX04522C PC (Asia Pacific) LNP Stat-Kon DX04522C is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: High Modulus, Electrically Conductive, Clean Compound System. Also .. |
|||
Linear Mold Shrinkage, Flow | 0.00060 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00060 - 0.0015 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Lexan_JK2500 PC+ABS LNP* Stat-kon* Lexan_JK2500 compound is a 20% carbon-fiber reinforced, nonhalogenated red phosporous-free, high-flow FR PC+ABS for EMI/RFI shielding. SE of 21 dB at 1.5 mm. |
|||
Linear Mold Shrinkage, Flow | 0.00060 cm/cm @Thickness 3.20 mm |
0.00060 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP DX13354 PC COPOLYMER (Asia Pacific) DX13354 is 30% glass fiber reinforced, impact modified and LDS functionalized polycarbonate resin. The features include LDS function, high flow, and good ductility. |
|||
Linear Mold Shrinkage, Flow | 0.00060 - 0.0026 cm/cm @Time 86400 sec |
0.00060 - 0.0026 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Verton NV0041EV_GY7E147 PC+ABS Preliminary data for 20% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.00060 cm/cm | 0.00060 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP WCP36 PBT (Europe-Africa-Middle East) LNP* LUBRICOMP* WCP36 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber, PTFE, Silicone. Added features include; Internally Lubricated, Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.00060 - 0.00080 cm/cm @Time 86400 sec |
0.00060 - 0.00080 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP QC008 PA6.10 LNP* THERMOCOMP* QC008 is a compound based on Nylon 6/10 containing 40% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.00060 - 0.0026 cm/cm @Time 86400 sec |
0.00060 - 0.0026 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Verton NV0081EV_GY7E149 PC+ABS Preliminary data for 40% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.00060 cm/cm @Time 86400 sec |
0.00060 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Europe-Africa-Middle East) LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.00060 cm/cm @Time 86400 sec |
0.00060 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Asia Pacific) LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.00060 cm/cm @Time 86400 sec |
0.00060 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Verton UX06451 BK8-312 PPA LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.00060 cm/cm @Time 86400 sec |
0.00060 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Verton UX06451 PPA LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.00060 cm/cm @Time 86400 sec |
0.00060 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Europe-Africa-Middle East) LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.00060 cm/cm @Time 86400 sec |
0.00060 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Asia Pacific) LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |