Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.00060 - 0.00090 cm/cm
0.00060 - 0.00090 in/in
ASTM D955 and ISO 294-4
Ravago Manufacturing Americas Hylon® N1213HL BK Nylon 6/6
Available in North America Filler: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantForm: Pellets Proces..
Linear Mold Shrinkage, Flow 0.00060 cm/cm
0.00060 in/in
Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
Lanxess Durethan® AKV 35 HR H2.0 901510 Nylon 66, Glass Fiber Reinforced
PA 66, 35% glass fibers, injection molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS.
Linear Mold Shrinkage, Flow 0.00060 cm/cm
0.00060 in/in
Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
Lanxess Durethan® BKV 130 GIT DUS008 900116 Nylon 6, Impact Modified
PA 6, 30% glass fibers, injection molding, impact modified, GIT/WITInformation provided by LANXESS.
Linear Mold Shrinkage, Flow 0.00060 - 0.00080 cm/cm

@Time 86400 sec
0.00060 - 0.00080 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP QCL34 PA6.10
LNP* LUBRICOMP* QCL34 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00060 - 0.00090 cm/cm

@Time 86400 sec
0.00060 - 0.00090 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP UX06427 PPA
LNP* LUBRICOMP* UX06427 is a compound based on PPA containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Heat Stabilized, Hot Water Moldable, Wear Resistant.
Linear Mold Shrinkage, Flow 0.00060 cm/cm
0.00060 in/in
ISO 294-4
Solvay Specialty Polymers Kalix® 5950 HFFR Polyamide, High Performance (HPPA), 50% Glass Fiber
Kalix® 5950 HFFR is a halogen-free, flame retardant (UL-94 V0 at 0.4 mm), highly reinforced polyamide material specifically formulated for high strength and stiffness applications where good impa..
Linear Mold Shrinkage, Flow 0.00060 - 0.00090 cm/cm

@Time 86400 sec
0.00060 - 0.00090 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DE004ER PC
LNP* STAT-KON* DE004ER is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added featuresof this material include: Electrically Conductive, Easy Molding, Mold Release.
Linear Mold Shrinkage, Flow 0.00060 - 0.00080 cm/cm

@Time 86400 sec
0.00060 - 0.00080 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DEF42 PC
LNP STAT-KON* DEF42 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00060 cm/cm

@Time 86400 sec
0.00060 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DX04522C PC (Asia Pacific)
LNP Stat-Kon DX04522C is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: High Modulus, Electrically Conductive, Clean Compound System. Also ..
Linear Mold Shrinkage, Flow 0.00060 - 0.0015 cm/cm

@Thickness 3.20 mm
0.00060 - 0.0015 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP STAT-KON Lexan_JK2500 PC+ABS
LNP* Stat-kon* Lexan_JK2500 compound is a 20% carbon-fiber reinforced, nonhalogenated red phosporous-free, high-flow FR PC+ABS for EMI/RFI shielding. SE of 21 dB at 1.5 mm.
Linear Mold Shrinkage, Flow 0.00060 cm/cm

@Thickness 3.20 mm
0.00060 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP DX13354 PC COPOLYMER (Asia Pacific)
DX13354 is 30% glass fiber reinforced, impact modified and LDS functionalized polycarbonate resin. The features include LDS function, high flow, and good ductility.
Linear Mold Shrinkage, Flow 0.00060 - 0.0026 cm/cm

@Time 86400 sec
0.00060 - 0.0026 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Verton NV0041EV_GY7E147 PC+ABS
Preliminary data for 20% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.00060 cm/cm
0.00060 in/in
SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP WCP36 PBT (Europe-Africa-Middle East)
LNP* LUBRICOMP* WCP36 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber, PTFE, Silicone. Added features include; Internally Lubricated, Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00060 - 0.00080 cm/cm

@Time 86400 sec
0.00060 - 0.00080 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP QC008 PA6.10
LNP* THERMOCOMP* QC008 is a compound based on Nylon 6/10 containing 40% Carbon Fiber. Added feature of this grade is: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.00060 - 0.0026 cm/cm

@Time 86400 sec
0.00060 - 0.0026 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Verton NV0081EV_GY7E149 PC+ABS
Preliminary data for 40% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.00060 cm/cm

@Time 86400 sec
0.00060 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Europe-Africa-Middle East)
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.
Linear Mold Shrinkage, Flow 0.00060 cm/cm

@Time 86400 sec
0.00060 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Asia Pacific)
LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.
Linear Mold Shrinkage, Flow 0.00060 cm/cm

@Time 86400 sec
0.00060 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Verton UX06451 BK8-312 PPA
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.00060 cm/cm

@Time 86400 sec
0.00060 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Verton UX06451 PPA
LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.00060 cm/cm

@Time 86400 sec
0.00060 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Europe-Africa-Middle East)
LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.
Linear Mold Shrinkage, Flow 0.00060 cm/cm

@Time 86400 sec
0.00060 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Asia Pacific)
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.