Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.021 cm/cm @Thickness 3.18 mm |
0.021 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Nymax™ 1200 IL Natural Polyamide 66 (Nylon 66) The Nymax® 1200 IL is an internally lubricated, unfilled nylon 6/6 designed for exceptional processing and mold release. This grade is intended primarily for injection molded applications where a g.. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm @Thickness 2.00 mm |
0.021 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 100P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin® 100P provides maximum toughness in the product line without modification. Delrin® 100P has improved pro.. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm @Thickness 2.00 mm |
0.021 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 127UVE NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 127UVE NC010 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information pro.. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm @Thickness 2.00 mm |
0.021 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 300CP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of processing and part performance.Information provided by DuPont Perf.. |
|||
Linear Mold Shrinkage, Flow | 0.021 - 0.024 cm/cm | 0.021 - 0.024 in/in | |
LATI Latilub 73/13-10ST POM, Silicone/PTFE Filled Self-lubricating product based on Polyoxymethylene (POM). Silicone / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | SABIC Method |
SABIC Innovative Plastics LNP Lubricomp WL0049XF PBT LNP* Lubricomp* WL0049 is a compound based on Polybutylene Terephalate resin containing PTFE and Flame Retardant. Added features include: Internally Lubricated, Flame Retardant.This data was suppl.. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm @Thickness 3.17 mm |
0.021 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Electrablend® POM C BK Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Conductive and CopolymerAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.021 - 0.027 cm/cm @Thickness 3.20 mm |
0.021 - 0.027 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ3001 PBT (Europe-Africa-Middle East) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Linear Mold Shrinkage, Flow | 0.021 - 0.024 cm/cm @Thickness 3.20 mm |
0.021 - 0.024 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® V2000DM PBT (Asia Pacific) Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
Linear Mold Shrinkage, Flow | 0.021 - 0.024 cm/cm @Thickness 3.20 mm |
0.021 - 0.024 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® V2000DM PBT (Europe-Africa-Middle East) Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm @Thickness 3.17 mm |
0.021 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® TPX-PVDF-03009 C Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral FillerFeatures: Low Shrinkage and Low Smoke EmissionInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | SABIC Method |
SABIC Innovative Plastics LNP Thermocomp MX96070 PP (Europe-Africa-Middle East) LNP* STARFLAM* MX96070 is a compound based on Polypropylene resin containing Flame Retardant. Added features include: Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middl.. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP IP004Z PA6.12 (Europe-Africa-Middle East) LNP* LUBRICOMP* IP004Z is a compound based on PA 6/12 resin containing PTFE, Silicone. Added features include : Internally Lubricated, Extrusion grade. |
|||
Linear Mold Shrinkage, Flow | 0.021 - 0.027 cm/cm @Thickness 3.20 mm |
0.021 - 0.027 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® IQ3001 PBT Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Linear Mold Shrinkage, Flow | 0.021 - 0.027 cm/cm @Thickness 3.20 mm |
0.021 - 0.027 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® V3004 PBT (Asia Pacific) Unfilled PBT modified with elastomer. Targeted for flexible hinge, automotive connectors, film applications. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | 0.125 in; ASTM D955 |
Chase Plastics CP Pryme® AH300 Acetal Homopolymer, Recycled Content Features: General purposeHigh heat resistanceGood chemical resistanceGood dimensional stabilityFatigue resistantLow frictionGrease resistantLow moisture absorptionOil resistantHigh rigiditySolvent r.. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 300CP NC010 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc.. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 100AF Acetal (POM)
(Unverified Data**) 20% Teflon® Fiber Filled High Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 100AF is a high viscosity acetal homopolymer containing 20% Teflon PTFE fibers. It is designed for a.. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | ISO Data |
BASF Ultraform H 2320 006 Q600 POM Ultraform H2320 006 is a high-molecular-weight grade of POM for injection molding. It conforms to FDA requirements of 21 CFR 177.2470. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | ISO Data |
BASF Ultraform N 2320 U03 UNC Q600 POM Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade. |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | ISO 2577 |
BASF Ultraform® N2520 L POM Description: Is a POM, product having reduced electric surface resistance.Information provided by BASF |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | ISO 2577 |
BASF Ultraform® N2770 K POM Description: Is a POM, injection-molding grade with improved wear characteristics for sliding elements.Information provided by BASF |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | ISO 2577 |
BASF Ultraform® S2320 0035 LEV POM Description: Is a POM, free-flowing and rapidly solidifying standard grade with reduced emission potential for injection molding.Information provided by BASF |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm | 0.021 in/in | ISO 2577 |
BASF Ultraform® S2320 003 PRO BK 00120 POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Linear Mold Shrinkage, Flow | 0.021 cm/cm @Thickness 2.00 mm |
0.021 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 300CP BK642 Acetal Homopolymer
(Unverified Data**) Delrin® 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of processing and part performance. This black is formulated to mainta.. |