Polymer Property : Linear Mold Shrinkage, Flow = 0.035 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.015 - 0.035 cm/cm

@Time 86400 sec
0.015 - 0.035 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Asia Pacific)
LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct..
Linear Mold Shrinkage, Flow 0.015 - 0.035 cm/cm

@Time 86400 sec
0.015 - 0.035 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Asia Pacific)
LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct..
Linear Mold Shrinkage, Flow 0.015 - 0.035 cm/cm

@Time 86400 sec
0.015 - 0.035 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Europe-Africa-Middle East)
LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct..
Linear Mold Shrinkage, Flow 0.015 - 0.035 cm/cm

@Time 86400 sec
0.015 - 0.035 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Europe-Africa-Middle East)
LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct..
Linear Mold Shrinkage, Flow 0.015 - 0.035 cm/cm

@Time 86400 sec
0.015 - 0.035 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer
LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.015 - 0.035 cm/cm

@Time 86400 sec
0.015 - 0.035 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer
LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Linear Mold Shrinkage, Flow 0.025 - 0.035 cm/cm

@Time 86400 sec
0.025 - 0.035 in/in

@Time 24.0 hour
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Linear Mold Shrinkage, Flow 0.019 - 0.035 cm/cm

@Time 86400 sec
0.019 - 0.035 in/in

@Time 24.0 hour
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Linear Mold Shrinkage, Flow 0.012 - 0.035 cm/cm

@Time 86400 sec
0.012 - 0.035 in/in

@Time 24.0 hour
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
Linear Mold Shrinkage, Flow 0.019 - 0.035 cm/cm

@Time 86400 sec
0.019 - 0.035 in/in

@Time 24.0 hour
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Linear Mold Shrinkage, Flow 0.028 - 0.035 cm/cm

@Time 86400 sec
0.028 - 0.035 in/in

@Time 24.0 hour
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Linear Mold Shrinkage, Flow 0.020 - 0.035 cm/cm

@Time 86400 sec
0.020 - 0.035 in/in

@Time 24.0 hour
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..